Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 50.2 MPa

@Strain 3.80 %,
Temperature 0.000 °C
7280 psi

@Strain 3.80 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500AF Acetal (POM)  (Unverified Data**)
20% Teflon® Fiber Filled Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500AF is a medium viscosity acetal homopolymer resin containing 20% Teflon PTFE fibers. It is desi..
Tensile Stress 50.2 MPa

@Strain 12.4 %,
Temperature 23.0 °C
7280 psi

@Strain 12.4 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 520MP NC010 Acetal (POM)  (Unverified Data**)
20% Teflon® Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 520MP is a medium viscosity acetal homopolymer containing 20% Teflon PTFE Micropowder. It is designe..
Tensile Stress 50.2 MPa

@Strain 1.80 %,
Temperature 40.0 °C
7280 psi

@Strain 1.80 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® 415HP NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
15% Glass Reinforced Polyethylene Terephthalate with Excellent Impact Resistance Rynite 415HP NC010 is a 15% glass reinforced modified polyethylene terephthalate improved for easy fast processing ov..
Tensile Stress 50.2 MPa

@Strain 1.89 %,
Temperature 120 °C
7280 psi

@Strain 1.89 %,
Temperature 248 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® 70G20HSL NC010 Nylon 66