Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 5.81 MPa @Strain 300 %, Temperature 23.0 °C |
843 psi @Strain 300 %, Temperature 73.4 °F |
Die C Flow 2 hr; ASTM D412 |
PolyOne Versalloy™ HC 9220-80 Thermoplastic Elastomer (TPE) Versalloy™ HC 9220-80 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr.. |
|||
Tensile Stress | 5.81 MPa @Strain 7.64 %, Temperature 150 °C |
843 psi @Strain 7.64 %, Temperature 302 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® BM6450XD BK560 Polybutylene Terephthalate (PBT)
(Unverified Data**)& Unreinforced Polybutylene Terephthalate Developed for Blow MoldingCrastin BM6450XD BK560 is an unreinforced supertough polybutylene terephthalate resin with very high viscosity for extrusion and blo.. |