Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 5.50 MPa @Strain 100 % |
798 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® S4670 TPE, PS Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesSporting GoodsInformation from Alliance Polymers & Services, Distributor of Nantong .. |
|||
Tensile Stress | 5.50 MPa @Strain 10.0 %, Temperature 23.0 °C |
798 psi @Strain 10.0 %, Temperature 73.4 °F |
ISO 527 (1BA bar) |
DuPont Performance Polymers Hytrel® HTR8223 BK320 TPC-ET
(Unverified Data**) Hytrel® HTR8223 BK320 is designed for blow molding or processing techniques requiring high melt viscosity. It has nominal hardness of 42D, is pigmented black with fine particle size carbon black, a.. |
|||
Tensile Stress | 5.50 MPa @Strain 100 % |
798 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® F7880 TPE, Fire Retardant Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Auto PartsSealsWire & Cable ElectronicsInformation from Alliance Polymers & Services, Distributor of Nantong Elastome.. |
|||
Tensile Stress | 5.50 MPa @Strain 0.110036 %, Time 36000 sec |
798 psi @Strain 0.110036 %, Time 10.0 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 73G30L NC010 Nylon 6
(Unverified Data**) 30% Glass Reinforced Polyamide 6Zytel 73G30L NC010 is a 30% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 5.50 MPa @Strain 0.0989091 %, Time 3600 sec |
798 psi @Strain 0.0989091 %, Time 1.00 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 73G30L NC010 Nylon 6
(Unverified Data**) 30% Glass Reinforced Polyamide 6Zytel 73G30L NC010 is a 30% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 5.50 MPa @Strain 0.134764 %, Time 3.60e+6 sec |
798 psi @Strain 0.134764 %, Time 1000 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 73G30L NC010 Nylon 6
(Unverified Data**) 30% Glass Reinforced Polyamide 6Zytel 73G30L NC010 is a 30% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 5.50 MPa @Strain 0.148364 %, Time 3.60e+7 sec |
798 psi @Strain 0.148364 %, Time 10000 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 73G30L NC010 Nylon 6
(Unverified Data**) 30% Glass Reinforced Polyamide 6Zytel 73G30L NC010 is a 30% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 5.50 MPa @Strain 0.121164 %, Time 360000 sec |
798 psi @Strain 0.121164 %, Time 100 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 73G30L NC010 Nylon 6
(Unverified Data**) 30% Glass Reinforced Polyamide 6Zytel 73G30L NC010 is a 30% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 5.50 MPa @Strain 0.0600 %, Temperature 150 °C |
798 psi @Strain 0.0600 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS95G50DH2 BK261 Nylon
(Unverified Data**) Zytel® PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology, only from DuPont providing exceptional Heat Resistance & High stiffness for automotive under hood.. |
|||
Tensile Stress | 5.50 MPa @Strain 10.0 % |
798 psi @Strain 10.0 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® HTR8223 BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 42 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 5.50 MPa @Strain 13.54 %, Temperature 60.0 °C |
798 psi @Strain 13.54 %, Temperature 140 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8223 BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 42 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | >= 5.50 MPa @Strain 100 % |
>= 798 psi @Strain 100 % |
ISO 37 |
Austin Novel Materials Texalan® 285A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech |
|||
Tensile Stress | >= 5.50 MPa @Strain 100 % |
>= 798 psi @Strain 100 % |
ISO 37 |
Austin Novel Materials Texalan® 482A Polyester-based TPU Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |