Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 46.44 MPa @Strain 0.360 %, Temperature 40.0 °C |
6736 psi @Strain 0.360 %, Temperature 104 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 73G50HSLA BK416 Nylon 6
(Unverified Data**) 50% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G50HSLA BK416 is a 50% glass fiber reinforced heat stabilized lubricated polyamide 6 resin for injection molding. It has an excellent surface.. |
|||
Tensile Stress | 46.44 MPa @Strain 10.0 %, Temperature 150 °C |
6736 psi @Strain 10.0 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 54G15HSLR NC010 Polyphthalamide (PPA)
(Unverified Data**) 15% Glass Reinforced Toughened PPA High Performance Polyamide Zytel HTN54G15HSLR NC010 is a 15% glass reinforced toughened heat stabilized hydrolysis resistant high performance polyamide resin. It i.. |