Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 45.0 MPa @Strain 1.00 %, Temperature 80.0 °C |
6530 psi @Strain 1.00 %, Temperature 176 °F |
|
Solvay TECHNYL® A 218 V30 PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Tensile Stress | 45.0 MPa @Strain 1.00 %, Temperature 80.0 °C |
6530 psi @Strain 1.00 %, Temperature 176 °F |
|
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, Conditioned Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Tensile Stress | 45.0 MPa @Strain 1.00 %, Temperature 120 °C |
6530 psi @Strain 1.00 %, Temperature 248 °F |
|
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, DRY Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Tensile Stress | 45.0 MPa @Strain 3.00 %, Temperature 200 °C |
6530 psi @Strain 3.00 %, Temperature 392 °F |
|
Solvay TECHNYL® A 218HP V35 PA66, 35% glass fiber, DRY Description: TECHNYL® A 218HP V35 is a polyamide 6.6, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits: The product of.. |
|||
Tensile Stress | 45.0 MPa @Strain 2.00 %, Temperature 200 °C |
6530 psi @Strain 2.00 %, Temperature 392 °F |
|
Solvay TECHNYL® A 218HP V50 PA66, 35% glass fiber, DRY Description: TECHNYL® A 218HP V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits: The product off.. |
|||
Tensile Stress | 45.0 MPa @Strain 2.00 %, Temperature 150 °C |
6530 psi @Strain 2.00 %, Temperature 302 °F |
|
Solvay TECHNYL® A 218W V33 Natural T PA66, 33% glass fiber, DRY Description: TECHNYL® A 218W V33 Nat T is a polyamide 66, reinforced with 33% of glass fiber, heat stabilized, for injection molding. This product is available in natural color.Benefits: The prod.. |
|||
Tensile Stress | 45.0 MPa @Strain 7.50 % |
6530 psi @Strain 7.50 % |
|
Solvay TECHNYL® A 221 PA66, Conditioned Description TECHNYL ® A 221 is an unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for fast cycles. It is available in natural colors. Benef.. |
|||
Tensile Stress | 45.0 MPa @Strain 0.500 % |
6530 psi @Strain 0.500 % |
|
Solvay TECHNYL® A 30 H1 V30 PA66, 30% glass fiber, DRY Description: TECHNYL® A 30H1 V30 is a brominated flame retardant polyamide 66, reinforced with 30% of glass fiber, for injection molding. This product is available in natural & black color.Benefi.. |
|||
Tensile Stress | 45.0 MPa @Strain 6.00 %, Temperature 80.0 °C |
6530 psi @Strain 6.00 %, Temperature 176 °F |
|
Solvay TECHNYL® A 548B2 V15 PA66, 15% glass fiber, DRY Description: TECHNYL® A 548B2 V15 is a polyamide 6.6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits: Th.. |
|||
Tensile Stress | 45.0 MPa @Strain 12.0 %, Temperature 80.0 °C |
6530 psi @Strain 12.0 %, Temperature 176 °F |
|
Solvay TECHNYL® A 548B2 V15 PA66, 15% glass fiber, DRY Description: TECHNYL® A 548B2 V15 is a polyamide 6.6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits: Th.. |
|||
Tensile Stress | 45.0 MPa @Strain 1.00 %, Temperature 60.0 °C |
6530 psi @Strain 1.00 %, Temperature 140 °F |
|
Solvay TECHNYL® A 60 G1 V25 PA66, 25% glass fiber, DRY Description: TECHNYL® A 60G1 V25 is a 25% GF reinforced organophosphorous flame retarded grade based on a patented high flow polyamide 66 resin. This product is heat stabilized and provides optim.. |
|||
Tensile Stress | 45.0 MPa @Strain 2.00 %, Temperature 120 °C |
6530 psi @Strain 2.00 %, Temperature 248 °F |
|
Solvay TECHNYL® A 218 MZ15 V 25 PA66, 25/15% glass/mineral fiber, Conditioned Description: TECHNYL® A 218 MZ15 V25 is a polyamide 66, reinforced with 25% of glass fiber and 15% of mineral filler, heat stabilized, for injection molding. This product is available in black co.. |
|||
Tensile Stress | 45.0 MPa @Strain 40.0 %, Temperature 80.0 °C |
6530 psi @Strain 40.0 %, Temperature 176 °F |
|
Solvay TECHNYL® A 205F PA66, DRY Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities.. |
|||
Tensile Stress | 45.0 MPa @Strain 1.84 %, Temperature 150 °C |
6530 psi @Strain 1.84 %, Temperature 302 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 530 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 30% Glass Reinforced Polyethylene Terephthalate Rynite 530 NC010 is a 30% glass fiber reinforced modified polyethylene terephthalate resin with an outstanding balance of strength stiffness and tough.. |
|||
Tensile Stress | 45.0 MPa @Strain 2.00 %, Temperature 150 °C |
6530 psi @Strain 2.00 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 53G50HSLR NC010 Polyphthalamide (PPA)
(Unverified Data**) 50% Glass Reinforced High Performance Polyamide with Improved Impact and Stiffness Zytel HTN53G50HSLR NC010 is a 50% glass reinforced heat stabilized lubricated high performance polyamide resin deve.. |
|||
Tensile Stress | 45.0 MPa @Strain 50.0 %, Temperature 23.0 °C |
6530 psi @Strain 50.0 %, Temperature 73.4 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® ST801AHS NC010 Nylon 66
(Unverified Data**) Zytel® ST801AHS NC010 is a Super Tough, high performance polyamide 66 resin. It offers outstanding molding performance in injection molding applications.Information provided by DuPont |
|||
Tensile Stress | 45.0 MPa @Strain 1.92 %, Temperature 90.0 °C |
6530 psi @Strain 1.92 %, Temperature 194 °F |
ISO 527 |
DuPont Performance Polymers Rynite® 408 NC010 PET Rynite® 408 NC010 is a 30% glass reinforced modified polyethylene terephthalate with improved impact resistance. Excellent balance of strength, stiffness, toughness, and temperature resistance.Inf.. |
|||
Tensile Stress | 45.0 MPa @Temperature 220 °C |
6530 psi @Temperature 428 °F |
|
BASF Ultramid® Endure D3G7 Glass-Fiber Reinforced Polyamide Description: Ultramid® Endure is a new, glass-fiber reinforced polyamide that combines excellent heat aging resistance with the good processing properties of PA 66. Ultramid® Endure can withstand .. |