Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 44.82 MPa @Strain 0.510 %, Temperature 40.0 °C |
6501 psi @Strain 0.510 %, Temperature 104 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 80G33HS1L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G33HS1L NC010 is a 33% glass fiber reinforced heat stabilized polyamide 66 resin with outstanding impact resistance developed usin.. |