Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 4.50 MPa @Strain 100 %, Thickness 2.00 mm |
653 psi @Strain 100 %, Thickness 0.0787 in |
Type 1, 200 mm/min; Flow; DIN 53504 |
PolyOne OnFlex™ BIO 5380A-E0006 Thermoplastic Elastomer (TPE) OnFlex™ BIO 5300 series thermoplastic elastomer compounds are soft thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% of renewable materi.. |
|||
Tensile Stress | 4.50 MPa @Strain 300 % |
653 psi @Strain 300 % |
ISO 37 |
PolyOne OnFlex™ S EH 80A-3S7005 Thermoplastic Elastomer (TPE) OnFlex™ S EH thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver a great cost/performance ratio in addition to t.. |
|||
Tensile Stress | 4.50 MPa @Strain 300 % |
653 psi @Strain 300 % |
ISO 37 |
PolyOne OnFlex™ S KE 60A-3S1725 Thermoplastic Elastomer (TPE) OnFlex™-S KE thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to a variety p.. |
|||
Tensile Stress | 4.50 MPa @Strain 300 % |
653 psi @Strain 300 % |
ASTM D412 |
Lubrizol ESTAGRIP® ST70A Polyether-Type Thermoplastic Polyurethane Features: Low durometer soft feel for excellent grip; outstanding adhesionUses: Injection Molding - OvermoldingAvailability: Americas, Europe, Middle East, Africa, India and AsiaInformation provided.. |
|||
Tensile Stress | 4.50 MPa @Strain 100 % |
653 psi @Strain 100 % |
ISO 527-1/-2 |
DSM Arnitel® XG6029 TPC-ET Extrusion Grade |
|||
Tensile Stress | 4.50 MPa @Strain 0.180 %, Temperature 90.0 °C |
653 psi @Strain 0.180 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® HR5315HFS BK591 Polybutylene Terephthalate (PBT)
(Unverified Data**) 15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate with Improved Processing Crastin HR5315HFS is a 15% glass fiber reinforced moderatley toughened hydrolysis resistant polybutylene.. |
|||
Tensile Stress | 4.50 MPa @Strain 0.180 %, Temperature 90.0 °C |
653 psi @Strain 0.180 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® HR5315HFS NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate with Improved Processing Crastin HR5315HFS is a 15% glass fiber reinforced moderatley toughened hydrolysis resistant polybutylene.. |
|||
Tensile Stress | 4.50 MPa @Strain 300 % |
653 psi @Strain 300 % |
ASTM D412 |
ExxonMobil Vistamaxx™ 3000 Propylene-based Elastomer Product Description: Vistamaxx 3000 propylene-based elastomer is an olefinic elastomer produced using ExxonMobil Chemical's EXXPOL™ Technology. It has moderate elastomeric properties, is easy to .. |
|||
Tensile Stress | 4.50 MPa @Strain 5.00 % |
653 psi @Strain 5.00 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® HTR8139BK Polyester Elastomer TPC-ET
(Unverified Data**) 44 Shore D Lubricated High Viscosity Polyester Elastomer Developed for Blow Molding Hytrel HTR8139BK is designed for blow molding or processing techniques requiring high melt viscosity. It has nomin.. |
|||
Tensile Stress | 4.50 MPa @Strain 200 %, Temperature 100 °C |
653 psi @Strain 200 %, Temperature 212 °F |
ISO 527 (1BA bar) |
DuPont Performance Polymers Hytrel® HTR8636 NC010 TPC-ET
(Unverified Data**) Hytrel® HTR8636 NC010 is a medium modulus Hytrel® grade with nominal durometer hardness of 40D. It contains non_discoloring stabilizer. It is specially suitable for extrusion processing.Informatio.. |
|||
Tensile Stress | >= 4.50 MPa @Strain 300 % |
>= 653 psi @Strain 300 % |
ISO 37 |
Austin Novel Materials Texalan® 270A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech |
|||
Tensile Stress | >= 4.50 MPa @Strain 300 % |
>= 653 psi @Strain 300 % |
ISO 37 |
Austin Novel Materials Texalan® 465A Polyester-based TPU Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Tensile Stress | >= 4.50 MPa @Strain 100 % |
>= 653 psi @Strain 100 % |
ISO 37 |
Austin Novel Materials Texalan® 470A Polyester-based TPU Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |