Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 38.1 MPa @Strain 6.10 %, Temperature 90.0 °C |
5530 psi @Strain 6.10 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 935 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 35% Glass Reinforced Polyethylene Terephthalate Rynite 935 NC010 is a 35% mica/glass reinforced modified polyethylene terephthalate resin with exceptionally low warpage excellent electrical properti.. |