Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 35.0 MPa @Strain 1.00 %, Temperature 120 °C |
5080 psi @Strain 1.00 %, Temperature 248 °F |
|
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, Conditioned Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Tensile Stress | 35.0 MPa @Strain 1.00 %, Temperature 200 °C |
5080 psi @Strain 1.00 %, Temperature 392 °F |
|
Solvay TECHNYL® A 218HP V35 PA66, 35% glass fiber, DRY Description: TECHNYL® A 218HP V35 is a polyamide 6.6, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits: The product of.. |
|||
Tensile Stress | 35.0 MPa @Strain 1.00 %, Temperature 100 °C |
5080 psi @Strain 1.00 %, Temperature 212 °F |
|
Solvay TECHNYL® A 218W V33 Natural T PA66, 33% glass fiber, DRY Description: TECHNYL® A 218W V33 Nat T is a polyamide 66, reinforced with 33% of glass fiber, heat stabilized, for injection molding. This product is available in natural color.Benefits: The prod.. |
|||
Tensile Stress | 35.0 MPa @Strain 1.00 % |
5080 psi @Strain 1.00 % |
|
Solvay TECHNYL® A 221 PA66, DRY Description TECHNYL ® A 221 is an unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for fast cycles. It is available in natural colors. Benef.. |
|||
Tensile Stress | 35.0 MPa @Strain 1.00 %, Temperature -40.0 °C |
5080 psi @Strain 1.00 %, Temperature -40.0 °F |
|
Solvay TECHNYL® A 548B2 V15 PA66, 15% glass fiber, DRY Description: TECHNYL® A 548B2 V15 is a polyamide 6.6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits: Th.. |
|||
Tensile Stress | 35.0 MPa @Strain 1.00 %, Temperature 23.0 °C |
5080 psi @Strain 1.00 %, Temperature 73.4 °F |
|
Solvay TECHNYL® A 548B2 V15 PA66, 15% glass fiber, DRY Description: TECHNYL® A 548B2 V15 is a polyamide 6.6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits: Th.. |
|||
Tensile Stress | 35.0 MPa @Strain 3.00 %, Temperature 80.0 °C |
5080 psi @Strain 3.00 %, Temperature 176 °F |
|
Solvay TECHNYL® A 548B2 V15 PA66, 15% glass fiber, DRY Description: TECHNYL® A 548B2 V15 is a polyamide 6.6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits: Th.. |
|||
Tensile Stress | 35.0 MPa @Strain 1.00 % |
5080 psi @Strain 1.00 % |
|
Solvay TECHNYL® B 50 H1 PA66/6, DRY Description: TECHNYL® B 50H1 is an unreinforced melamine cyanurate flame retarded copolyamide 66/6. This product has been heat stabilized and is suitable for injection molding. This product is av.. |
|||
Tensile Stress | 35.0 MPa @Strain 8.50 %, Temperature 23.0 °C |
5080 psi @Strain 8.50 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100ST NC010 Acetal (POM)
(Unverified Data**) Super Toughened High Viscosity Acetal Homopolymer Delrin 100ST NC010 is a super tough high viscosity acetal homopolymer grade with superior impact resistance. It is designed for highly stressed part.. |
|||
Tensile Stress | 35.0 MPa @Strain 13.0 %, Temperature 0.000 °C |
5080 psi @Strain 13.0 %, Temperature 32.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC1600 NC010 Nylon 1010 Plasticized Toughened UV Stabilized Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1600 NC010 is a renewable sourced Polyamide 1010 containing a minimum of 60% renewably sourced.. |
|||
Tensile Stress | 35.0 MPa @Strain 3.00 %, Temperature 140 °C |
5080 psi @Strain 3.00 %, Temperature 284 °F |
ISO 527 |
BASF Ultradur B 4300 G4 20% Glass Filled PBT Ultradur B4300 G4 is an easy flowing injection molding PBT with 20% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |
|||
Tensile Stress | 35.0 MPa @Strain 0.500 %, Time 3600 sec |
5080 psi @Strain 0.500 %, Time 1.00 hour |
ISO 899-1 |
BASF Ultraform N 2200 G53 UNC Q600 25% Glass Filled POM Ultraform N2200 G53 UNC Q600 is a 25% glass fiber reinforced POM injection molding grade with enhanced stiffness and toughness. |
|||
Tensile Stress | >= 35.0 MPa @Strain 300 % |
>= 5080 psi @Strain 300 % |
ISO 37 |
Austin Novel Materials Texalan® 564D Polyether-based TPU Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech |
|||
Tensile Stress | 35.0 MPa @Strain 2.00 %, Temperature 160 °C |
5080 psi @Strain 2.00 %, Temperature 320 °F |
ISO 527 |
BASF Ultrason S 3010 PSU Ultrason S 3010 is an unreinforced, higher viscosity injection molding and extrusion PSU grade, tougher and with improved chemical resistance. It conforms to FDA requirements of 21 CFR 177.1655. |
|||
Tensile Stress | 35.0 MPa @Temperature 160 °C |
5080 psi @Temperature 320 °F |
|
BASF Ultrason® P 3010 PPSU Unreinforced Polyphenylsulfone Description: Medium viscosity injection-molding and extrusion grade with good toughness and chemical resistance (stress crack resistance), resistant against superheated steam. The property profile m.. |
|||
Tensile Stress | 35.0 MPa @Strain 0.220 %, Temperature 40.0 °C |
5080 psi @Strain 0.220 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 545 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 45% Glass Reinforced Polyethylene Terephthalate Rynite 545 NC010 is a 45% glass reinforced modified polyethylene terephthalate with greater strength and stiffness excellent dimensional stability and.. |
|||
Tensile Stress | 35.0 MPa @Strain 50.0 % |
5080 psi @Strain 50.0 % |
dry; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4208 black 9992 PA612-I Product description: Grilamid XE 4208 black 9992 is a semiflexible high viscosity, plasticized, high impact and highly heat resistant polyamide 612 (PA612) extrusion grade. Unique properties of Gril.. |
|||
Tensile Stress | 35.0 MPa @Strain 4.77 %, Temperature 120 °C |
5080 psi @Strain 4.77 %, Temperature 248 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Crastin® HR5315HF NC010 PBT
(Unverified Data**) Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis.. |
|||
Tensile Stress | 35.0 MPa @Strain 3.00 %, Time 3.60e+6 sec |
5080 psi @Strain 3.00 %, Time 1000 hour |
140°C; DIN 50014-23/50-2 |
BASF Ultradur B 4300 G6 30% Glass Filled PBT Ultradur B4300 G6 is an easy flowing injection molding PBT with 30% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |
|||
Tensile Stress | 35.0 MPa @Strain 2.00 %, Time 3.60e+6 sec |
5080 psi @Strain 2.00 %, Time 1000 hour |
100°C; DIN 50014-23/50-2 |
BASF Ultradur B 4300 G6 30% Glass Filled PBT Ultradur B4300 G6 is an easy flowing injection molding PBT with 30% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |