Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 30.0 MPa @Strain 1.00 %, Temperature 120 °C |
4350 psi @Strain 1.00 %, Temperature 248 °F |
|
Solvay TECHNYL® A 218 V30 PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Tensile Stress | 30.0 MPa @Strain 1.00 % |
4350 psi @Strain 1.00 % |
|
Solvay TECHNYL® A 548B V15 PA66, 15% glass fiber, DRY Description: TECHNYL® A 548B V15 is a copolyamide 6.6/6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits:.. |
|||
Tensile Stress | 30.0 MPa @Strain 3.00 %, Temperature 120 °C |
4350 psi @Strain 3.00 %, Temperature 248 °F |
|
Solvay TECHNYL® A 548B2 V15 PA66, 15% glass fiber, DRY Description: TECHNYL® A 548B2 V15 is a polyamide 6.6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits: Th.. |
|||
Tensile Stress | 30.0 MPa @Strain 12.0 %, Temperature 200 °C |
4350 psi @Strain 12.0 %, Temperature 392 °F |
|
Solvay TECHNYL® A 548B2 V15 PA66, 15% glass fiber, DRY Description: TECHNYL® A 548B2 V15 is a polyamide 6.6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits: Th.. |
|||
Tensile Stress | 30.0 MPa @Strain 1.00 %, Temperature 140 °C |
4350 psi @Strain 1.00 %, Temperature 284 °F |
|
Solvay TECHNYL® A 60 G1 V25 PA66, 25% glass fiber, DRY Description: TECHNYL® A 60G1 V25 is a 25% GF reinforced organophosphorous flame retarded grade based on a patented high flow polyamide 66 resin. This product is heat stabilized and provides optim.. |
|||
Tensile Stress | 30.0 MPa @Strain 160 %, Temperature 80.0 °C |
4350 psi @Strain 160 %, Temperature 176 °F |
|
Solvay TECHNYL® eXten D 437P PA6.10 Description: TECHNYL® eXten D 437P is a high viscosity, unfilled, plasticized, UV and heat stabilized PA6.10 for extrusion applications. Technyl® eXten D 437P is a partially biosourced materia.. |
|||
Tensile Stress | 30.0 MPa @Strain 1.00 %, Temperature 80.0 °C |
4350 psi @Strain 1.00 %, Temperature 176 °F |
|
Solvay TECHNYL® A 218 MZ15 V 25 PA66, 25/15% glass/mineral fiber, Conditioned Description: TECHNYL® A 218 MZ15 V25 is a polyamide 66, reinforced with 25% of glass fiber and 15% of mineral filler, heat stabilized, for injection molding. This product is available in black co.. |
|||
Tensile Stress | 30.0 MPa @Strain 50.0 % |
4350 psi @Strain 50.0 % |
dry; ISO 527-1/-2 |
EMS-Grivory Grivory® 2D 25 W 20 HL X black 9992 PA612-I Product Description: Grilamid 2D 25 W 20 HL X black 9992 is a semi-flexible high viscosity, plasticized, high impact and highly heat resistant polyamide 612 (PA612) grade. Unique properties of Gril.. |
|||
Tensile Stress | 30.0 MPa @Strain 50.0 % |
4350 psi @Strain 50.0 % |
dry; ISO 527-1/-2 |
EMS-Grivory Grivory® 2D 25 W 20 X black PA612-I Product Description: Grilamid 2D 25 W 20 X black 9992 is a semi-flexible high viscosity, plasticized, high impact, heat and UV resistant extrusion grade based on polyamide 612 (PA612). Unique proper.. |
|||
Tensile Stress | 30.0 MPa @Strain 50.0 % |
4350 psi @Strain 50.0 % |
dry; ISO 527-1/-2 |
EMS-Grivory Grivory® 2D 25 W 20 X nat PA612-I Product Description: Grilamid 2D 25 W 20 X natural 9992 is a semi-flexible high viscosity, plasticized, high impact, heat and UV resistant extrusion grade based on polyamide 612 (PA612). Unique pro.. |
|||
Tensile Stress | 30.0 MPa @Strain 50.0 % |
4350 psi @Strain 50.0 % |
dry; ISO 527-1/-2 |
EMS-Grivory Grivory® BRZ 247 W PA6 Product description: Grilon BRZ 247 W is a heat stabilized, high viscosity, impact modified and plasticized PA6 extrusion grade. Grilon BRZ 247 W has the following important properties: High flexibi.. |
|||
Tensile Stress | 30.0 MPa @Strain 50.0 % |
4350 psi @Strain 50.0 % |
dry; ISO 527-1/-2 |
EMS-Grivory Grivory® BRZ 347 W PA6 Product description: Grilon BRZ 347 W is a heat stabilized, high viscosity, impact modified and plasticized PA6 extrusion grade. Grilon BRZ 347 W has the following important properties: High flexibi.. |
|||
Tensile Stress | 30.0 MPa @Strain 50.0 % |
4350 psi @Strain 50.0 % |
conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4180 black 9992 PA1010 Product description: Grilamid XE 4180 black 9992 is a unreinforced, high viscosity, plasticized, high impact resistant polyamide 1010 (PA1010) extrusion grade. Grilamid XE 4180 black 9992 is highly .. |
|||
Tensile Stress | 30.0 MPa @Strain 50.0 % |
4350 psi @Strain 50.0 % |
dry; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4180 black 9992 PA1010 Product description: Grilamid XE 4180 black 9992 is a unreinforced, high viscosity, plasticized, high impact resistant polyamide 1010 (PA1010) extrusion grade. Grilamid XE 4180 black 9992 is highly .. |
|||
Tensile Stress | 30.0 MPa @Strain 50.0 % |
4350 psi @Strain 50.0 % |
conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4180 nat PA1010 Product description: Grilamid XE 4180 natural is a unreinforced, high viscosity, plasticized, high impact resistant polyamide 1010 (PA1010) extrusion grade. Grilamid XE 4180 NATURAL is highly resist.. |
|||
Tensile Stress | 30.0 MPa @Strain 50.0 % |
4350 psi @Strain 50.0 % |
dry; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4180 nat PA1010 Product description: Grilamid XE 4180 natural is a unreinforced, high viscosity, plasticized, high impact resistant polyamide 1010 (PA1010) extrusion grade. Grilamid XE 4180 NATURAL is highly resist.. |
|||
Tensile Stress | 30.0 MPa @Strain 4.17 %, Time 3.60e+6 sec |
4350 psi @Strain 4.17 %, Time 1000 hour |
isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® S600F20UV WT660 Polybutylene Terephthalate (PBT) Unreinforced UV Stabilized Polybutylene Terephthalate Crastin S600F20 NC010 is an unreinforced lubricated medium viscosity polybutylene terephthalate resin for injection molding.Information provided.. |
|||
Tensile Stress | 30.0 MPa @Strain 0.510 %, Time 360000 sec |
4350 psi @Strain 0.510 %, Time 100 hour |
isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK603 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Crastin SK603 NC010 is a 20% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |
|||
Tensile Stress | 30.0 MPa @Strain 0.250 %, Temperature -20.0 °C |
4350 psi @Strain 0.250 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK605 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Crastin SK605 NC010 is a 30% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |
|||
Tensile Stress | 30.0 MPa @Strain 0.400 %, Time 3.60e+6 sec |
4350 psi @Strain 0.400 %, Time 1000 hour |
isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK645FR NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK645FR is a flame retardant 30% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.7.. |
|||
Tensile Stress | 30.0 MPa @Strain 0.210 %, Temperature 40.0 °C |
4350 psi @Strain 0.210 %, Temperature 104 °F |
ISO 527 |
DuPont Performance Polymers Rynite® FR543 NC010 PET Rynite® FR543 NC010 is a flame retardant, 43% glass reinforced polyethylene terephthalate. Has a 155C temperature index that is equivalent to many thermosets. Recognized by UL as UL94V-0 at 0.8mm.. |
|||
Tensile Stress | 30.0 MPa @Strain 1.08 %, Temperature 40.0 °C |
4350 psi @Strain 1.08 %, Temperature 104 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® FR70M30V0 NC010 Nylon 66
(Unverified Data**) 30% Mineral Reinforced Flame Retardant Polyamide 66 Zytel FR70M30V0 NC010 is a 30% mineral reinforced flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performa.. |
|||
Tensile Stress | 30.0 MPa @Strain 1.61 %, Temperature -40.0 °C |
4350 psi @Strain 1.61 %, Temperature -40.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS 3261TL NC010 Nylon 610
(Unverified Data**) Toughened Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3261TL NC010 is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient by.. |
|||
Tensile Stress | 30.0 MPa @Strain 0.500 %, Temperature 23.0 °C |
4350 psi @Strain 0.500 %, Temperature 73.4 °F |
|
Akro-Plastic Akroloy® PA GF 50 (2706) PA 6.6 & PA6I/6T Dry, 50% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |
|||
Tensile Stress | 30.0 MPa @Strain 10.0 %, Temperature 140 °C |
4350 psi @Strain 10.0 %, Temperature 284 °F |
ISO 527 |
BASF Ultradur B 4300 G2 10% Glass Filled PBT Ultradur B4300 G2 is an easy flowing injection molding PBT with 10% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |
|||
Tensile Stress | 30.0 MPa @Strain 1.00 %, Temperature 40.0 °C |
4350 psi @Strain 1.00 %, Temperature 104 °F |
ISO 527 |
BASF Ultradur B 4300 G2 10% Glass Filled PBT Ultradur B4300 G2 is an easy flowing injection molding PBT with 10% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |
|||
Tensile Stress | 30.0 MPa @Temperature 160 °C |
4350 psi @Temperature 320 °F |
|
BASF Ultrason® P 3010 PPSU Unreinforced Polyphenylsulfone Description: Medium viscosity injection-molding and extrusion grade with good toughness and chemical resistance (stress crack resistance), resistant against superheated steam. The property profile m.. |
|||
Tensile Stress | >= 30.0 MPa @Strain 100 % |
>= 4350 psi @Strain 100 % |
ISO 37 |
Austin Novel Materials Texalan® 572D Polyether-based TPU Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech |
|||
Tensile Stress | 30.0 MPa @Strain 2.00 %, Time 3.60e+6 sec |
4350 psi @Strain 2.00 %, Time 1000 hour |
140°C; DIN 50014-23/50-2 |
BASF Ultradur B 4300 G6 30% Glass Filled PBT Ultradur B4300 G6 is an easy flowing injection molding PBT with 30% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |
|||
Tensile Stress | 30.0 MPa @Strain 1.00 % |
4350 psi @Strain 1.00 % |
|
Solvay TECHNYL® A 218 PA66, 33% glass fiber, DRY Standard viscosity, heat stabilized for injection molding. It is available in natural and black colors.Benefits: This product offers all the primary properties of unreinforced polyamide 66. In addit.. |