Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 3.90 MPa @Strain 100 % |
566 psi @Strain 100 % |
ISO 37 |
PolyOne OnFlex™ S KA 80A-3S1770 Thermoplastic Elastomer (TPE) OnFlex™-S KA thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to polyamide p.. |
|||
Tensile Stress | 3.90 MPa @Strain 300 % |
566 psi @Strain 300 % |
ISO 37 |
PolyOne OnFlex™ S KE 50A-3S1731 Thermoplastic Elastomer (TPE) OnFlex™-S KE thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to a variety p.. |
|||
Tensile Stress | 3.90 MPa @Strain 100 %, Temperature 23.0 °C |
566 psi @Strain 100 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7680-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7680-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop.. |
|||
Tensile Stress | 3.90 MPa @Strain 100 %, Temperature 23.0 °C |
566 psi @Strain 100 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7680-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7680-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Tensile Stress | 3.90 MPa @Strain 10.0 % |
566 psi @Strain 10.0 % |
ISO 527-1/-2 |
DSM Arnitel® EM400-BP TPC-ET 34 Shore D, Injection Molding or Extrusion Grade |
|||
Tensile Stress | 3.90 MPa @Strain 5.68 %, Temperature 90.0 °C |
566 psi @Strain 5.68 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® DYM250S BK472 TPC-ET+PBT
(Unverified Data**) Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsHytrel DYM250S BK472 is a medium modulus resin suited for injection molding of Air Bag Depl.. |
|||
Tensile Stress | 3.90 MPa @Strain 0.0700 %, Temperature 150 °C |
566 psi @Strain 0.0700 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS93G35DH1 BK261 Nylon 6
(Unverified Data**) Zytel® PLS93G35DH1 BK261 is a 35% glass reinforced PA6 using SHIELD Technology, only from DuPont, it provides exceptional welding resistance & retention over time thanks to excellent Heat Resistanc.. |