Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 3.66 MPa @Strain 100 % |
531 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® S4465 TPE, PS Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesSporting GoodsInformation from Alliance Polymers & Services, Distributor of Nantong .. |
|||
Tensile Stress | 3.66 MPa @Strain 100 % |
531 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® S4665 TPE, PS Overmold Characteristics: Excellent slip resistanceSoft touchGood weather and heat resistanceEasy processingWide range of hardnessExceptional colorabilityTypical Applications: ConsumerElectronicsHealthcareIn.. |
|||
Tensile Stress | 3.66 MPa @Strain 32.97 %, Temperature 90.0 °C |
531 psi @Strain 32.97 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4056 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 3.66 MPa @Strain 0.0500 %, Temperature 180 °C |
531 psi @Strain 0.0500 %, Temperature 356 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 92G35DH2 BK083 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide with DuPont Zytel HTN92G35DH2 BK083 is a 35% glass reinforced high performance polyamide resin using DuPont SHIELD Technology with high flow and e.. |
|||
Tensile Stress | 3.66 MPa @Strain 0.0800 %, Temperature 220 °C |
531 psi @Strain 0.0800 %, Temperature 428 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS90G30DR BK099 Nylon 66
(Unverified Data**) Zytel® PLS90G30DR BK099 is a 30% glass reinforced PA66 nylon resin having superior resistance to hot engine coolant. It is particularly suitable for automotive Radiator End Tanks and other parts in.. |
|||
Tensile Stress | 3.66 MPa @Strain 0.170 %, Temperature -40.0 °C |
531 psi @Strain 0.170 %, Temperature -40.0 °F |
50%RH; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® RS LC1600 BK385 Nylon 1010
(Unverified Data**) Zytel® RS LC1600 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 60% renewably sourced ingredient by weight. It is flexible, toughened, plasticized, UV and heat stabilized and s.. |
|||
Tensile Stress | 3.66 MPa @Strain 14.45 %, Temperature 60.0 °C |
531 psi @Strain 14.45 %, Temperature 140 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® G4074 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4074 is a low modulus grade with nominal hardness of 40D. It contains discoloring stabilizer. It can be process.. |
|||
Tensile Stress | 3.66 MPa @Strain 59.34 %, Temperature 150 °C |
531 psi @Strain 59.34 %, Temperature 302 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8223 BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 42 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers |