Mechanical Properties Metric English Comments
Tensile Stress 3.61 MPa

@Strain 100 %
524 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® P2875 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress >= 3.61 MPa

@Strain 50.0 %
>= 524 psi

@Strain 50.0 %
ASTM D412 Method A
Seals Eastern 7042U Fluorocarbon-Elastomer
Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Type..