Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 3.30 MPa @Strain 100 %, Thickness 2.00 mm |
479 psi @Strain 100 %, Thickness 0.0787 in |
Type 1, 200 mm/min Across Flow; DIN 53504 |
PolyOne OnFlex™ BIO 5370A-E0004 Thermoplastic Elastomer (TPE) OnFlex™-Bio 5300 series thermoplastic elastomer compounds are soft thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% of renewable materi.. |
|||
Tensile Stress | 3.30 MPa @Strain 300 % |
479 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® P1770 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 3.30 MPa @Strain 51.73 %, Temperature 100 °C |
479 psi @Strain 51.73 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4056 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 3.30 MPa @Strain 0.0600 %, Temperature 220 °C |
479 psi @Strain 0.0600 %, Temperature 428 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS95G50DH2 BK261 Nylon
(Unverified Data**) Zytel® PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology, only from DuPont providing exceptional Heat Resistance & High stiffness for automotive under hood.. |
|||
Tensile Stress | 3.30 MPa @Strain 64.05 %, Temperature 120 °C |
479 psi @Strain 64.05 %, Temperature 248 °F |
ISO 527 |
DuPont Performance Polymers Hytrel® G4078W TPC-ET
(Unverified Data**) Hytrel® G4078W is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like inject.. |
|||
Tensile Stress | 3.30 MPa @Strain 100 %, Temperature 100 °C |
479 psi @Strain 100 %, Temperature 212 °F |
ISO 527 (1BA bar) |
DuPont Performance Polymers Hytrel® HTR8636 NC010 TPC-ET
(Unverified Data**) Hytrel® HTR8636 NC010 is a medium modulus Hytrel® grade with nominal durometer hardness of 40D. It contains non_discoloring stabilizer. It is specially suitable for extrusion processing.Informatio.. |
|||
Tensile Stress | 3.30 MPa @Strain 10.0 % |
479 psi @Strain 10.0 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® RS 40F3 NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Renewably Sourced High Flow Polyester Elastomer Developed for Injection Molding Hytrel RS 40F3 NC010 is a high flow low modulus grade containing at least 50% renewably sourced ingredients.. |