Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 3.22 MPa @Strain 42.0 %, Temperature 90.0 °C |
467 psi @Strain 42.0 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4056 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 3.22 MPa @Strain 85.58 %, Temperature 120 °C |
467 psi @Strain 85.58 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4068FG Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 3.22 MPa @Strain 58.08 %, Temperature 120 °C |
467 psi @Strain 58.08 %, Temperature 248 °F |
ISO 527 |
DuPont Performance Polymers Hytrel® G4078W TPC-ET
(Unverified Data**) Hytrel® G4078W is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like inject.. |