Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 26.86 MPa @Strain 1.18 %, Temperature -40.0 °C |
3896 psi @Strain 1.18 %, Temperature -40.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC3090 NC010 Nylon 610
(Unverified Data**) Unreinforced Renewably Sourced High Viscosity Polyamide 610 Developed for Extrusion Zytel RS LC3090 NC010 is a renewable sourced polyamide 610 containing a miniumu of 60% renewably sourced ingredien.. |
|||
Tensile Stress | 26.86 MPa @Strain 23.59 %, Temperature 90.0 °C |
3896 psi @Strain 23.59 %, Temperature 194 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 153HSL NC010 Nylon 612
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 612 Information provided by DuPont Performance Polymers |