Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 250 MPa @Strain 2.00 %, Temperature 0.000 °C |
36300 psi @Strain 2.00 %, Temperature 32.0 °F |
|
Solvay TECHNYLSTARâ„¢ AFX 218 V60 PA6, 60% glass filled, Conditioned Description: TECHNYLSTARâ„¢ AFX 218 V60 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 60% of glass fiber, for injection molding.Benefits: Due.. |
|||
Tensile Stress | 250 MPa @Diameter 25.0 - 50.0 mm, Strain 0.200 % |
36300 psi @Diameter 0.984 - 1.97 in, Strain 0.200 % |
|
United Cast Bar Unibar 400-15 As Cast Continuously Cast Spheroidal Graphite Iron Offers superior machinability combined with good impact, fatigue, electrical conductivity and magnetic permeability. Noise and vibration damping are good in this grade.Unibar 400-15 is not recommend.. |
|||
Tensile Stress | 250 MPa @Diameter 55.0 - 100 mm, Strain 0.200 % |
36300 psi @Diameter 2.17 - 3.94 in, Strain 0.200 % |
|
United Cast Bar Unibar 400-15 As Cast Continuously Cast Spheroidal Graphite Iron Offers superior machinability combined with good impact, fatigue, electrical conductivity and magnetic permeability. Noise and vibration damping are good in this grade.Unibar 400-15 is not recommend.. |
|||
Tensile Stress | 250 MPa @Diameter 25.0 - 50.0 mm, Strain 0.200 % |
36300 psi @Diameter 0.984 - 1.97 in, Strain 0.200 % |
|
United Cast Bar Unibar 400-15 Fully Annealed Continuously Cast Spheroidal Graphite Iron Offers superior machinability combined with good impact, fatigue, electrical conductivity and magnetic permeability. Noise and vibration damping are good in this grade.Unibar 400-15 is not recommend.. |
|||
Tensile Stress | 250 MPa @Diameter 55.0 - 100 mm, Strain 0.200 % |
36300 psi @Diameter 2.17 - 3.94 in, Strain 0.200 % |
|
United Cast Bar Unibar 400-15 Fully Annealed Continuously Cast Spheroidal Graphite Iron Offers superior machinability combined with good impact, fatigue, electrical conductivity and magnetic permeability. Noise and vibration damping are good in this grade.Unibar 400-15 is not recommend.. |