Mechanical Properties Metric English Comments
Tensile Stress 2.39 MPa

@Strain 100 %
347 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® C4960M TPE, Transparent
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf..
Tensile Stress 2.39 MPa

@Strain 300 %
347 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® P3750 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 2.39 MPa

@Strain 5.61 %,
Temperature 0.000 °C
347 psi

@Strain 5.61 %,
Temperature 32.0 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4068FG Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 2.39 MPa

@Strain 0.810 %,
Temperature 150 °C
347 psi

@Strain 0.810 %,
Temperature 302 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 444AHS BK152 Nylon 66  (Unverified Data**)
Toughened Heat Stabilized Polyamide 66 Zytel 444AHS is a toughened heat stabilized black polyamide 66 resin for injection molding. It is a high flow processing friendly material.Information provided..
Copyright © lookpolymers.com All Rights Reserved