Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 2.22 MPa @Strain 300 % |
322 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® C4750 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Tensile Stress | 2.22 MPa @Strain 300 % |
322 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® N8860 TPE, Nylon Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Auto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInformation from Alliance Polymers & Se.. |
|||
Tensile Stress | 2.22 MPa @Strain 300 % |
322 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® P1957TB TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 2.22 MPa @Strain 100 % |
322 psi @Strain 100 % |
Average; ASTM D412 Method A |
Seals Eastern 5722A Fluorocarbon-Elastomer Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Exce.. |
|||
Tensile Stress | 2.22 MPa @Strain 0.100 %, Temperature 23.0 °C |
322 psi @Strain 0.100 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN FE8200 NC010 Polyphthalamide (PPA)
(Unverified Data**) Unreinforced Toughened PPA High Performance Polyamide Zytel HTNFE8200 NC010 is an unreinforced toughened heat stabilized lubricated high performance polyamide resin for injection molding. It is also.. |