Mechanical Properties Metric English Comments
Tensile Stress 2.16 MPa

@Strain 100 %
313 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® P1860D TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 2.16 MPa

@Strain 300 %
313 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® P3850 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 2.16 MPa

@Strain 63.22 %,
Temperature 120 °C
313 psi

@Strain 63.22 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4056 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 2.16 MPa

@Strain 7.12 %,
Temperature 60.0 °C
313 psi

@Strain 7.12 %,
Temperature 140 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4068FG Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 2.16 MPa

@Strain 7.18 %,
Temperature 60.0 °C
313 psi

@Strain 7.18 %,
Temperature 140 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4068 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers
Tensile Stress 2.16 MPa

@Strain 16.56 %,
Temperature 120 °C
313 psi

@Strain 16.56 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® G4074 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4074 is a low modulus grade with nominal hardness of 40D. It contains discoloring stabilizer. It can be process..
Copyright © lookpolymers.com All Rights Reserved