Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 19.0 MPa @Strain 3.00 %, Temperature 200 °C |
2760 psi @Strain 3.00 %, Temperature 392 °F |
|
Solvay TECHNYL® A 548B2 V15 PA66, 15% glass fiber, DRY Description: TECHNYL® A 548B2 V15 is a polyamide 6.6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits: Th.. |
|||
Tensile Stress | 19.0 MPa @Strain 20.0 %, Temperature 150 °C |
2760 psi @Strain 20.0 %, Temperature 302 °F |
|
Solvay TECHNYL® A 205F PA66, Conditioned Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities.. |
|||
Tensile Stress | 19.0 MPa @Strain 10.0 %, Temperature 120 °C |
2760 psi @Strain 10.0 %, Temperature 248 °F |
|
Solvay TECHNYL® A 205F PA66, DRY Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities.. |
|||
Tensile Stress | 19.0 MPa @Strain 100 % |
2760 psi @Strain 100 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® 6356 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 19.0 MPa @Strain 300 % |
2760 psi @Strain 300 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® HTR8223 BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 42 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 19.0 MPa @Strain 50.0 % |
2760 psi @Strain 50.0 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® HTR8441 BK316 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 19.0 MPa @Strain 300 % |
2760 psi @Strain 300 % |
ASTM D412 |
Alliance Polymers Zythane™ 4090A Thermoplastic Polyurethane Elastomer Zythane™ 4090A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Tensile Stress | 19.0 MPa @Time 3600 sec, Strain 1.00 % |
2760 psi @Time 1.00 hour, Strain 1.00 % |
ISO 899-1 |
BASF Ultraform N 2320 003 UNC Q600 POM Ultraform N 2320 003 UNC Q600 is a rapidly solidifying grade of POM for injection molding. Contains a mold release agent. |
|||
Tensile Stress | >= 19.0 MPa @Strain 100 % |
>= 2760 psi @Strain 100 % |
ISO 37 |
Austin Novel Materials Texalan® 264D Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech |
|||
Tensile Stress | >= 19.0 MPa @Strain 100 % |
>= 2760 psi @Strain 100 % |
ISO 37 |
Austin Novel Materials Texalan® 372D Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech |
|||
Tensile Stress | 19.0 MPa @Strain 5.00 %, Temperature 150 °C |
2760 psi @Strain 5.00 %, Temperature 302 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 11C40 NC010 Nylon 66
(Unverified Data**) 40% Mineral Reinforced Polyamide 66 Minlon 11C40 NC010 is a 40% mineral reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |