Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 18.9 MPa @Strain 0.250 %, Temperature 0.000 °C |
2740 psi @Strain 0.250 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9020 NC010 PBT+ASA
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9020 NC010 is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. .. |