Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 153.48 MPa @Strain 1.89 %, Temperature -20.0 °C |
22260 psi @Strain 1.89 %, Temperature -4.00 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 80G33HS1L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G33HS1L NC010 is a 33% glass fiber reinforced heat stabilized polyamide 66 resin with outstanding impact resistance developed usin.. |