Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 15.93 MPa @Strain 0.270 %, Temperature 23.0 °C |
2310 psi @Strain 0.270 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G13HS1L NC010 Nylon 66
(Unverified Data**) 13% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G13HS1L NC010 is a 13% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perfor.. |