Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 13.39 MPa @Strain 7.45 %, Temperature 60.0 °C |
1942 psi @Strain 7.45 %, Temperature 140 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 7246 Polyester Elastomer TPC-ET
(Unverified Data**) 72 Shore D High Performance Polyester Elastomer.Information provided by DuPont Performance Polymers |