Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 13.14 MPa @Strain 60.18 %, Temperature 100 °C |
1906 psi @Strain 60.18 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 7246 Polyester Elastomer TPC-ET
(Unverified Data**) 72 Shore D High Performance Polyester Elastomer.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 13.14 MPa @Strain 0.270 %, Temperature 175 °C |
1906 psi @Strain 0.270 %, Temperature 347 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN FR52G30NH NC010 Polyphthalamide (PPA)
(Unverified Data**) 30% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide Zytel HTNFR52G30NH NC010 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin. It.. |