Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 121.5 MPa @Strain 1.40 %, Temperature 23.0 °C |
17620 psi @Strain 1.40 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G33HS1L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G33HS1L NC010 is a 33% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perfor.. |
|||
Tensile Stress | 121.5 MPa @Strain 1.21618 %, Temperature -40.0 °C |
17620 psi @Strain 1.21618 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK615SF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK615SF is a 30% glass fiber reinforced low viscosity polybutylene terephthalate for injecti.. |