Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 11.15 MPa @Strain 36.1 %, Temperature 120 °C |
1617 psi @Strain 36.1 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 7246 Polyester Elastomer TPC-ET
(Unverified Data**) 72 Shore D High Performance Polyester Elastomer.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 11.15 MPa @Strain 0.210 %, Temperature 180 °C |
1617 psi @Strain 0.210 %, Temperature 356 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 92G35DH2 BK083 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide with DuPont Zytel HTN92G35DH2 BK083 is a 35% glass reinforced high performance polyamide resin using DuPont SHIELD Technology with high flow and e.. |