Mechanical Properties Metric English Comments
Tensile Stress 10.49 MPa

@Strain 0.200 %,
Temperature 150 °C
1521 psi

@Strain 0.200 %,
Temperature 302 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN FR52G30NH BK337 Polyphthalamide (PPA)  (Unverified Data**)
30% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide Zytel HTNFR52G30NH BK337 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin. It..
Tensile Stress 10.49 MPa

@Strain 4.49 %,
Temperature 90.0 °C
1521 psi

@Strain 4.49 %,
Temperature 194 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS 3261TL NC010 Nylon 610  (Unverified Data**)
Toughened Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3261TL NC010 is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient by..
Copyright © lookpolymers.com All Rights Reserved