Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 0.951 MPa @Strain 300 %, Temperature 23.0 °C |
138 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ VDT 4132 Thermoplastic Elastomer (TPE) Versaflex™ VDT 4132 is designed to create vibration damping. - Excellent Vibration DampingRear = 350-370F Middle = 375-400F Front = 375-400F Nozzle = 365-380F Screw speed = 100-500rpmPurge thorough.. |
|||
Tensile Stress | 0.951 MPa @Strain 100 % |
138 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® P3935T TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | >= 0.951 MPa @Strain 50.0 % |
>= 138 psi @Strain 50.0 % |
ASTM D412 Method A |
Seals Eastern 5722A Fluorocarbon-Elastomer Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Exce.. |