Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 0.590 MPa @Strain 100 % |
85.6 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® P3925T TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 0.590 MPa @Strain 0.160 %, Temperature 90.0 °C |
85.6 psi @Strain 0.160 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® BM6450XD BK560 Polybutylene Terephthalate (PBT)
(Unverified Data**)& Unreinforced Polybutylene Terephthalate Developed for Blow MoldingCrastin BM6450XD BK560 is an unreinforced supertough polybutylene terephthalate resin with very high viscosity for extrusion and blo.. |
|||
Tensile Stress | 0.590 MPa @Strain 0.240 %, Temperature 40.0 °C |
85.6 psi @Strain 0.240 %, Temperature 104 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4556 Polyester Elastomer TPC-ET
(Unverified Data**) 45 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 0.590 MPa @Strain 0.230 %, Temperature -40.0 °C |
85.6 psi @Strain 0.230 %, Temperature -40.0 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8223 BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 42 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers |