| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Dart Drop Total Energy | 60.1 J/cm @Temperature 23.0 °C |
0.113 ft-lb/mil @Temperature 73.4 °F |
Procedure A, C.125; ASTM D4226 |
| PolyOne Geon™ Vinyl Rigid Extrusion 87560 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
| Dart Drop Total Energy | 60.1 J/cm @Temperature 23.0 °C |
0.113 ft-lb/mil @Temperature 73.4 °F |
Procedure A, C.125; ASTM D4226 |
| PolyOne Geon™ Vinyl Rigid Extrusion L0148 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: Finished part testing is required for ASTM E-84 certification. Note: The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by Po.. |
|||
| Dart Drop Total Energy | 60.1 J/cm @Temperature 23.0 °C |
0.113 ft-lb/mil @Temperature 73.4 °F |
Procedure A, C.125; ASTM D4226 |
| PolyOne Geon™ Vinyl Rigid Extrusion L9620 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
| Dart Drop Total Energy | 60.1 J/cm @Temperature 23.0 °C |
0.113 ft-lb/mil @Temperature 73.4 °F |
Procedure B, C.125; ASTM D4226 |
| PolyOne Geon™ Vinyl Dry Blend E7506 Polyvinyl Chloride, Rigid (PVC, Rigid) Geon E7506 is recommended for whites and light pastel colors only. Performs well in extrusion blow molding and high rate fencing capstock applications.Physical properties based on Geon E7506 white 1.. |
|||