Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 4.14 GPa @Thickness 1.57 mm |
600 ksi @Thickness 0.0620 in |
CW; ASTM D229 |
Industrial Laminates/Norplex NP159 Synthetic Fabric
(discontinued **) Description: Woven aramid fiber fabric combined with high temperature phenolic resin. With a proper post baking procedure, NP159 will withstand continuous operation at 200° C. Material becomes brit.. |