Polymer Property : Modulus of Elasticity = 32100 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 221 GPa

@Temperature 20.0 °C
32100 ksi

@Temperature 68.0 °F
Dynamic
Haynes 75 Nickel Alloy Sheet, Annealed at 1925°F (1050°C)
Haynes alloy 75 is a solution-strengthened nickel-chromium alloy with moderate strength to 1200°F (650°C). It is principally used in low stress elevated temperature applications requiring reas..
Modulus of Elasticity 221 GPa

@Temperature 22.0 °C
32100 ksi

@Temperature 71.6 °F
Special Metals INCONEL® alloy 740 Precipitation-Hardenable Ni-Cr-Co Superalloy
INCONEL® alloy 740 is a nickel-chromium-cobalt alloy developed by Special Metals Corporation. The alloy is age hardenable by the precipitation of a gamma prime second phase. Potential applicati..