Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 205 GPa @Temperature 200 °C |
29700 ksi @Temperature 392 °F |
Dynamic |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Bar, Hot Rolled and Solution Annealed HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Modulus of Elasticity | 205 GPa @Temperature 200 °C |
29700 ksi @Temperature 392 °F |
Dynamic |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Modulus of Elasticity | 205 GPa @Temperature 20.0 °C |
29700 ksi @Temperature 68.0 °F |
|
Haynes Hastelloy® X alloy, sheet Solid-solution-strengthened with very good high-temperature strength and very good resistance to oxidizing environments up to about 1095°C, and good carburization resistance. Applications includ.. |
|||
Modulus of Elasticity | 205 GPa @Temperature 400 °C |
29700 ksi @Temperature 752 °F |
Dynamic |
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Modulus of Elasticity | 205 GPa @Temperature 400 °C |
29700 ksi @Temperature 752 °F |
Dynamic |
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Modulus of Elasticity | 205 GPa @Temperature 400 °C |
29700 ksi @Temperature 752 °F |
Dynamic |
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) Sheet Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Modulus of Elasticity | 205 GPa @Temperature 400 °C |
29700 ksi @Temperature 752 °F |
Dynamic |
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Modulus of Elasticity | 205 GPa @Temperature 400 °C |
29700 ksi @Temperature 752 °F |
Dynamic |
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate, Age-hardened Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Modulus of Elasticity | 205 GPa @Temperature 400 °C |
29700 ksi @Temperature 752 °F |
Dynamic |
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate, Annealed Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Modulus of Elasticity | 205 GPa @Temperature 400 °C |
29700 ksi @Temperature 752 °F |
Dynamic |
Haynes Hastelloy® C-22HS™ Nickel Alloy Sheet, Cold-rolled, Solution Annealed Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Modulus of Elasticity | 205 GPa @Temperature 400 °C |
29700 ksi @Temperature 752 °F |
Dynamic |
Haynes Hastelloy® C-22HS™ Nickel Alloy Sheet, Cold-rolled, Solution Annealed, Age-hardened Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Modulus of Elasticity | 205 GPa @Temperature 400 °C |
29700 ksi @Temperature 752 °F |
Dynamic |
Haynes Hastelloy® C-22HS™ Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Modulus of Elasticity | 205 GPa @Temperature 200 °C |
29700 ksi @Temperature 392 °F |
Dynamic |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Modulus of Elasticity | 205 GPa @Temperature 200 °C |
29700 ksi @Temperature 392 °F |
Dynamic |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Sheet, Cold Rolled and Solution Annealed HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Modulus of Elasticity | 205 GPa @Temperature 200 °C |
29700 ksi @Temperature 392 °F |
Dynamic |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Modulus of Elasticity | 205 GPa @Temperature 20.0 °C |
29700 ksi @Temperature 68.0 °F |
|
EDRO #3 Prehardened Mold Quality P20 Alloy Steel EDRO #3™ is a vacuum-degassed, ladle refined, Cr-Ni-Mo- alloyed steel which is supplied in the hardened and tempered condition. EDRO #3™ is manufactured to consistently high quality standards with.. |
|||
Modulus of Elasticity | 205 GPa @Temperature 400 °C |
29700 ksi @Temperature 752 °F |
Dynamic |
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed, Age-hardened Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately doubl.. |
|||
Modulus of Elasticity | 205 GPa @Temperature 400 °C |
29700 ksi @Temperature 752 °F |
Dynamic |
Haynes Hastelloy® C-22HS™ Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately doubl.. |
|||
Modulus of Elasticity | 205 GPa @Temperature 200 °C |
29700 ksi @Temperature 392 °F |
Dynamic |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Plate, Hot Rolled and Solution Annealed HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing spe.. |
|||
Modulus of Elasticity | 205 GPa @Temperature 200 °C |
29700 ksi @Temperature 392 °F |
Dynamic |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing spe.. |