Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 197 GPa @Temperature 20.0 °C |
28500 ksi @Temperature 68.0 °F |
|
EDRO UltraChem® #15 Precipitation Hardening Stainless Mold Steel Ultrachem® is a chromium-nickel precipitation-hardening stainless steel, a modified PH alloy grade, which is characterized by: exceptional corrosion resistance, uniform hardness in all dimensions, .. |
|||
Modulus of Elasticity | 197 GPa @Temperature 20.0 °C |
28500 ksi @Temperature 68.0 °F |
|
EDRO UltraChem® ESR #16 Precipitation Hardening Stainless Mold Steel Ultrachem ESR® is a chromium-nickel precipitation-hardening stainless steel, a modified PH alloy grade, which is characterized by exceptional polishability, exceptional corrosion resistance, unifor.. |