Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 17.2 GPa @Thickness 1.57 mm |
2500 ksi @Thickness 0.0620 in |
LW; ASTM D229 |
Industrial Laminates/Norplex NP310HT Cotton Fabric Description: Canvas machining grade for structural and mechanical applications. Better impact strength than phenolic paper grades. MIL-I-24768/16. Designed to meet GE specification A19B15B1Thickness.. |
|||
Modulus of Elasticity | 17.2 GPa @Thickness 1.57 mm |
2500 ksi @Thickness 0.0620 in |
LW; ASTM D229 |
Industrial Laminates/Norplex NP424 Laminate Description: Composite material composed of woven glass fabric surfaces and paper core combined with epoxy resin. Primarily used in the printed circuit board industry. Easy punching and excellent el.. |