Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 16.5 GPa @Thickness 1.57 mm |
2400 ksi @Thickness 0.0620 in |
CW; ASTM D229 |
Industrial Laminates/Norplex NP130 Glass Fabric Description: Woven glass fabric combined with a halogenated epoxy resin system. Produced to printed circuit board quality standards. Flame retardant, meets UL-94 flammability classification V-0.Thic.. |
|||
Modulus of Elasticity | 16.5 GPa @Thickness 1.57 mm |
2400 ksi @Thickness 0.0620 in |
CW; ASTM D229 |
Industrial Laminates/Norplex NP310HT Cotton Fabric Description: Canvas machining grade for structural and mechanical applications. Better impact strength than phenolic paper grades. MIL-I-24768/16. Designed to meet GE specification A19B15B1Thickness.. |