Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | >= 96.0 GPa @Temperature 20.0 °C |
>= 13900 ksi @Temperature 68.0 °F |
|
PEAK Werkstoff DISPAL S263 Aluminum Alloy, AlSi25Cu3Fe3Ni3MgCoTi, Condition T6 Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
Modulus of Elasticity | >= 96.0 GPa @Temperature 20.0 °C |
>= 13900 ksi @Temperature 68.0 °F |
|
PEAK Werkstoff DISPAL S263 Aluminum Alloy, AlSi25Cu3Fe3Ni3MgCoTi, Condition T4 Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
Modulus of Elasticity | >= 96.0 GPa @Temperature 20.0 °C |
>= 13900 ksi @Temperature 68.0 °F |
Condition T4 (Quenching in water at 80C) |
PEAK Werkstoff DISPAL S270 Aluminum Alloy, AlSi25Fe4Ni3CuMgMnCrTi, Condition T4 Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |