Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | >= 80.0 GPa @Temperature 150 °C |
>= 11600 ksi @Temperature 302 °F |
|
PEAK Werkstoff DISPAL S260 Aluminum Alloy, AlSi25Cu4Mg, Condition T7 Heat Treatment Condition T7 (Quenching in water at RT)Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allo.. |
|||
Modulus of Elasticity | >= 80.0 GPa @Temperature 200 °C |
>= 11600 ksi @Temperature 392 °F |
|
PEAK Werkstoff DISPAL S263 Aluminum Alloy, AlSi25Cu3Fe3Ni3MgCoTi, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |