Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 217 GPa @Temperature 25.0 °C |
31500 ksi @Temperature 77.0 °F |
Dynamic |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Bar, Hot Rolled and Solution Annealed HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Modulus of Elasticity | 217 GPa @Temperature 25.0 °C |
31500 ksi @Temperature 77.0 °F |
Dynamic |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Modulus of Elasticity | 217 GPa @Temperature 25.0 °C |
31500 ksi @Temperature 77.0 °F |
Dynamic |
Haynes 282® Nickel Alloy Autogenously Welded Sheet Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Modulus of Elasticity | 217 GPa @Temperature 25.0 °C |
31500 ksi @Temperature 77.0 °F |
Dynamic |
Haynes 282® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Modulus of Elasticity | 217 GPa @Temperature 25.0 °C |
31500 ksi @Temperature 77.0 °F |
Dynamic |
Haynes 282® Nickel Alloy Sheet, Plate and Bar, Solution Annealed Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Modulus of Elasticity | 217 GPa @Temperature 25.0 °C |
31500 ksi @Temperature 77.0 °F |
Dynamic |
Haynes 282® Nickel Alloy Sheet, Solution Annealed and Age-hardened Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Modulus of Elasticity | 217 GPa @Temperature 25.0 °C |
31500 ksi @Temperature 77.0 °F |
Dynamic |
Haynes 282® Nickel Alloy Sheet, Solution Annealed and Cold Worked Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Modulus of Elasticity | 217 GPa @Temperature 25.0 °C |
31500 ksi @Temperature 77.0 °F |
Dynamic |
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Modulus of Elasticity | 217 GPa @Temperature 25.0 °C |
31500 ksi @Temperature 77.0 °F |
Dynamic |
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Modulus of Elasticity | 217 GPa @Temperature 25.0 °C |
31500 ksi @Temperature 77.0 °F |
Dynamic |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Modulus of Elasticity | 217 GPa @Temperature 25.0 °C |
31500 ksi @Temperature 77.0 °F |
Dynamic |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Sheet, Cold Rolled and Solution Annealed HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Modulus of Elasticity | 217 GPa @Temperature 25.0 °C |
31500 ksi @Temperature 77.0 °F |
Dynamic |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Modulus of Elasticity | 217 GPa @Thickness 12.7 mm, Temperature 21.1 °C |
31500 ksi @Thickness 0.500 in, Temperature 70.0 °F |
(Heat treated at 1066°C (1950°F), rapid quenched, plate) |
HP Alloys Alloy B-2, Solution Treated, 10% Cold Worked Solution Treated, 10% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
Modulus of Elasticity | 217 GPa @Thickness 12.7 mm, Temperature 21.1 °C |
31500 ksi @Thickness 0.500 in, Temperature 70.0 °F |
(Heat treated at 1066°C (1950°F), rapid quenched, plate) |
HP Alloys Alloy B-2, Solution Treated, 20% Cold Worked Solution Treated, 20% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
Modulus of Elasticity | 217 GPa @Thickness 12.7 mm, Temperature 21.1 °C |
31500 ksi @Thickness 0.500 in, Temperature 70.0 °F |
(Heat treated at 1066°C (1950°F), rapid quenched, plate) |
HP Alloys Alloy B-2, Solution Treated, 30% Cold Worked Solution Treated, 30% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
Modulus of Elasticity | 217 GPa @Thickness 12.7 mm, Temperature 21.1 °C |
31500 ksi @Thickness 0.500 in, Temperature 70.0 °F |
(Heat treated at 1066°C (1950°F), rapid quenched, plate) |
HP Alloys Alloy B-2, Solution Treated, 40% Cold Worked Solution Treated, 40% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
Modulus of Elasticity | 217 GPa @Temperature 25.0 °C |
31500 ksi @Temperature 77.0 °F |
Dynamic |
Haynes 282® Nickel Alloy Sheet, Gamma-Prime Strengthened Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b.. |
|||
Modulus of Elasticity | 217 GPa @Temperature 25.0 °C |
31500 ksi @Temperature 77.0 °F |
Dynamic |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Plate, Hot Rolled and Solution Annealed HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing spe.. |
|||
Modulus of Elasticity | 217 GPa @Temperature 25.0 °C |
31500 ksi @Temperature 77.0 °F |
Dynamic |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing spe.. |
|||
Modulus of Elasticity | 217 GPa @Thickness 12.7 mm, Temperature 21.1 °C |
31500 ksi @Thickness 0.500 in, Temperature 70.0 °F |
(Heat treated at 1066°C (1950°F), rapid quenched, plate) |
HP Alloys Alloy B-2, Solution Treated, 50% Cold Worked Solution Treated, 50% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
Modulus of Elasticity | 217 GPa @Temperature 25.0 °C |
31500 ksi @Temperature 77.0 °F |
Dynamic |
Haynes 282® Nickel Alloy Plate, Solution Annealed and Age-Hardened Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b.. |