Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 170 GPa @Temperature 649 °C |
24700 ksi @Temperature 1200 °F |
Dynamic |
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2025°F (1107°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Modulus of Elasticity | 170 GPa @Temperature 649 °C |
24700 ksi @Temperature 1200 °F |
Dynamic |
Haynes Hastelloy® G-35® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Modulus of Elasticity | 170 GPa @Temperature 649 °C |
24700 ksi @Temperature 1200 °F |
Dynamic |
Haynes Hastelloy® G-35® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Modulus of Elasticity | 170 GPa @Temperature 649 °C |
24700 ksi @Temperature 1200 °F |
Dynamic |
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2075°F (1135°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Modulus of Elasticity | 170 GPa @Temperature 649 °C |
24700 ksi @Temperature 1200 °F |
Dynamic |
Haynes Hastelloy® G-35® Nickel Alloy Sheet, Annealed at 2075°F (1135°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is.. |
|||
Modulus of Elasticity | 170 GPa @Temperature 649 °C |
24700 ksi @Temperature 1200 °F |
Dynamic |
Haynes Hastelloy® G-35® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is.. |
|||
Modulus of Elasticity | 170 GPa @Temperature 649 °C |
24700 ksi @Temperature 1200 °F |
Dynamic |
Haynes Hastelloy® G-35® Nickel Alloy Bar, Annealed at 2075°F (1135°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is.. |