Polymer Property : Modulus of Elasticity = 16.5 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 16.5 GPa

@Thickness 1.57 mm
2400 ksi

@Thickness 0.0620 in
CW; ASTM D229
Industrial Laminates/Norplex NP130 Glass Fabric
Description: Woven glass fabric combined with a halogenated epoxy resin system. Produced to printed circuit board quality standards. Flame retardant, meets UL-94 flammability classification V-0.Thic..
Modulus of Elasticity 16.5 GPa

@Thickness 1.57 mm
2400 ksi

@Thickness 0.0620 in
CW; ASTM D229
Industrial Laminates/Norplex NP310HT Cotton Fabric
Description: Canvas machining grade for structural and mechanical applications. Better impact strength than phenolic paper grades. MIL-I-24768/16. Designed to meet GE specification A19B15B1Thickness..