| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched | 3.43 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
6.43 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
| LG Chemical MP211 ABS, Low Gloss, Metal Plating Feature: Injection Molding, High Flow, Metal PlatingApplication: Decorative Parts (Home Appliance Door Handle Etc)CAS No. 9003-56-9 and 9003-54-7Information provided by LG Chemical |
|||
| Izod Impact, Notched | 3.43 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
6.43 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
| LG Chemical RS656H ABS, Chemical Resistance to Cyclopentane Feature: Extrusion Molding, General Purpose, Chemical Resistance to CyclopentaneApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
| Izod Impact, Notched | 3.43 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
6.43 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
| LG Chemical RS800D ABS, High Impact, Chemical Resistance to HCFC Feature: Extrusion Molding, High Impact, Chemical Resistance to HCFCApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
| Izod Impact, Notched | 3.43 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
6.43 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
| LG Chemical RS800M ABS, High Modulus, Chemical Resistance to HCFC Feature: Extrusion Molding, High Modulus, Chemical Resistance to HCFCApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
| Izod Impact, Notched | 3.43 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
6.43 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
ASTM D256 |
| Samsung Cheil Industries Infino® WP-1098 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
| Izod Impact, Notched | 3.43 J/cm @Thickness 3.17 mm |
6.43 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Samsung Cheil Industries Starex® NA-0660I ABS, Unreinforced Anti-Bacteria Grade Nano-silver high flowability antibacterial ABS that can be used in notebook keyboardsInformation provided by Samsung Cheil Industries. |
|||
| Izod Impact, Notched | 3.43 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
6.43 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
ASTM D256 |
| Samsung Cheil Industries Infino® WP-1098 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
| Izod Impact, Notched | 3.43 J/cm @Thickness 3.17 mm |
6.43 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Samsung Cheil Industries Starex® NA-0660I ABS, Unreinforced Anti-Bacteria Grade Nano-silver high flowability antibacterial ABS that can be used in notebook keyboardsInformation provided by Samsung Cheil Industries. |
|||
| Izod Impact, Notched | 3.43 J/cm @Temperature 0.000 °C |
6.43 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
| SCG Chemicals EL-Leneâ„¢ H1000P High Density Polyethylene Pipe Resin Key Characteristics: Good processing, high thermal stabilityRecommended Applications: Water pipes, conduit, sewage drainage pipesInformation provided by SCG Chemicals |
|||
| Izod Impact, Notched | 3.43 J/cm @Temperature 23.0 °C |
6.43 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
| E-Polymers SEPAZ® LC50 PP Copolymer LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
| Izod Impact, Notched | 3.43 J/cm @Temperature -30.0 °C |
6.43 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
| E-Polymers SEPAZ® LC50 PP Copolymer LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
| Izod Impact, Notched | 3.43 J/cm @Thickness 6.40 mm |
6.43 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
| Bhansali Engineering Abstron HI40I ABS Injection Molding Grade Automotive applications -Super High Impact , High Rigidity, PaintableInformation provided by Bhansali |
|||
| Izod Impact, Notched | 3.43 J/cm @Temperature 23.0 °C |
6.43 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
| E-Polymers SEPAZ® LB50 PA6 LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
| Izod Impact, Notched | 3.43 J/cm @Temperature -30.0 °C |
6.43 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
| E-Polymers SEPAZ® LB50 PA6 LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
| Izod Impact, Notched | 3.43 J/cm @Temperature 23.0 °C |
6.43 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
| E-Polymers SEPAZ® LB60 PA6 LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
| Izod Impact, Notched | 3.43 J/cm @Temperature -30.0 °C |
6.43 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
| E-Polymers SEPAZ® LB60 PA6 LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
| Izod Impact, Notched | 3.43 J/cm @Thickness 6.40 mm |
6.43 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
| Bhansali Engineering Abstron HI40I ABS Injection Molding Grade Automotive applications -Super High Impact , High Rigidity, PaintableInformation provided by Bhansali |
|||