Mechanical Properties Metric English Comments
Izod Impact, Notched 2.35 J/cm
<br>@Thickness 3.20 mm,<br> Temperature 23.0 °C
4.41 ft-lb/in
<br>@Thickness 0.126 in,<br> Temperature 73.4 °F
ASTM D256
LG Chemical AF312A ABS, Flame Retardant
Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical..
Izod Impact, Notched 2.35 J/cm
<br>@Thickness 6.40 mm,<br> Temperature 23.0 °C
4.41 ft-lb/in
<br>@Thickness 0.252 in,<br> Temperature 73.4 °F
ASTM D256
LG Chemical HF380NS ABS, High Flow, General Anti-Static
Feature: Injection Molding, High Flow, General Anti-StaticApplication: Electric & Electronic Products, Miscellaneous goods)CAS No. 9003-56-9Information provided by LG Chemical
Izod Impact, Notched 2.35 J/cm
<br>@Thickness 3.20 mm,<br> Temperature 23.0 °C
4.41 ft-lb/in
<br>@Thickness 0.126 in,<br> Temperature 73.4 °F
ASTM D256
LG Chemical HF380NS ABS, High Flow, General Anti-Static
Feature: Injection Molding, High Flow, General Anti-StaticApplication: Electric & Electronic Products, Miscellaneous goods)CAS No. 9003-56-9Information provided by LG Chemical
Izod Impact, Notched 2.35 J/cm
<br>@Thickness 6.40 mm,<br> Temperature 23.0 °C
4.41 ft-lb/in
<br>@Thickness 0.252 in,<br> Temperature 73.4 °F
ASTM D256
LG Chemical HG173 ABS, High Surface Gloss
Feature: Injection Molding, High Surface GlossApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical
Izod Impact, Notched 2.35 J/cm
<br>@Thickness 6.40 mm,<br> Temperature 23.0 °C
4.41 ft-lb/in
<br>@Thickness 0.252 in,<br> Temperature 73.4 °F
ASTM D256
LG Chemical LG749W ABS, Low Gloss, Heat Resistance
Feature: Injection Molding, Low Gloss, Heat ResistanceApplication: Automotive Interior Housing (Glove Cover, Door S/W Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by..
Izod Impact, Notched 2.35 J/cm
<br>@Thickness 6.40 mm,<br> Temperature 23.0 °C
4.41 ft-lb/in
<br>@Thickness 0.252 in,<br> Temperature 73.4 °F
ASTM D256
LG Chemical PI642G ABS, General Purpose, High Modulus
Feature: Extrusion Molding, General Purpose, High ModulusApplication: Pipe fittingCAS No. 9003-56-9Information provided by LG Chemical
Izod Impact, Notched 2.35 J/cm
<br>@Thickness 3.20 mm,<br> Temperature 23.0 °C
4.41 ft-lb/in
<br>@Thickness 0.126 in,<br> Temperature 73.4 °F
ASTM D256
LG Chemical XR401B ABS, High Flow, Heat Resistance
Feature: Injection Molding, High Flow, Heat ResistanceApplication: Automotives Exterior Housing (Side Mirror Housing, Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information p..
Izod Impact, Notched 2.35 J/cm
<br>@Thickness 3.17 mm
4.41 ft-lb/in
<br>@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Starex® LX-0987EXS ABS, Unreinforced Metallic-Look
Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries.
Izod Impact, Notched 2.35 J/cm
<br>@Thickness 6.35 mm
4.41 ft-lb/in
<br>@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Starex® QU-0191S ABS, Unreinforced Extrusion Grade
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 2.35 J/cm
<br>@Thickness 3.17 mm
4.41 ft-lb/in
<br>@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Starex® SR-0305 ABS, Unreinforced Heat Resistant
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 2.35 J/cm
<br>@Thickness 3.17 mm
4.41 ft-lb/in
<br>@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Starex® LX-0987EXS ABS, Unreinforced Metallic-Look
Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries.
Izod Impact, Notched 2.35 J/cm
<br>@Thickness 6.35 mm
4.41 ft-lb/in
<br>@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Starex® QU-0191S ABS, Unreinforced Extrusion Grade
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 2.35 J/cm
<br>@Thickness 3.17 mm
4.41 ft-lb/in
<br>@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Starex® SR-0305 ABS, Unreinforced Heat Resistant
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 2.35 J/cm
<br>@Thickness 6.40 mm
4.41 ft-lb/in
<br>@Thickness 0.252 in
ASTM D256
Bhansali Engineering Abstron IM-11 ABS Injection Molding Grade
High Impact, High Rigidity, High Fatigue, Low Flow, PaintableInformation provided by Bhansali
Izod Impact, Notched 2.35 J/cm
<br>@Thickness 6.40 mm
4.41 ft-lb/in
<br>@Thickness 0.252 in
ASTM D-256
Bhansali Engineering Abstron IM-11BM ABS Injection Molding Grade
High Impact Strength, Medium Flow, High Fatigue ResistanceInformation provided by Bhansali
Izod Impact, Notched 2.35 J/cm
<br>@Thickness 6.40 mm
4.41 ft-lb/in
<br>@Thickness 0.252 in
ASTM D-256
Bhansali Engineering Abstron IM-14G ABS Very High Rigidity Injection Molding Grade
Very High Rigidity, High Gloss, Medium Impact with excellent other mechanical propertiesInformation provided by Bhansali
Izod Impact, Notched 2.35 J/cm
<br>@Thickness 3.20 mm
4.41 ft-lb/in
<br>@Thickness 0.126 in
ASTM D256
Bhansali Engineering Abstron KU602 ABS Heat Resistant
High ImpactInformation provided by Bhansali
Izod Impact, Notched 2.35 J/cm
<br>@Thickness 3.20 mm
4.41 ft-lb/in
<br>@Thickness 0.126 in
ASTM D256
Bhansali Engineering Abstron KU602L ABS Heat Resistant
High rigidityInformation provided by Bhansali
Izod Impact, Notched 2.35 J/cm
<br>@Thickness 3.20 mm
4.41 ft-lb/in
<br>@Thickness 0.126 in
ASTM D256
Bhansali Engineering Abstron KU603 ABS Heat Resistant
High Impact, High RigidityInformation provided by Bhansali
Izod Impact, Notched 2.35 J/cm
<br>@Thickness 6.40 mm
4.41 ft-lb/in
<br>@Thickness 0.252 in
ASTM D-256
Bhansali Engineering Abstron IM-11BM ABS Injection Molding Grade
High Impact Strength, Medium Flow, High Fatigue ResistanceInformation provided by Bhansali
Izod Impact, Notched 2.35 J/cm
<br>@Thickness 3.20 mm
4.41 ft-lb/in
<br>@Thickness 0.126 in
ASTM D256
Bhansali Engineering Abstron KU602L ABS Heat Resistant
High rigidityInformation provided by Bhansali
Izod Impact, Notched 2.35 J/cm
<br>@Thickness 6.40 mm
4.41 ft-lb/in
<br>@Thickness 0.252 in
ASTM D256
Bhansali Engineering Abstron IM-11 ABS Injection Molding Grade
High Impact, High Rigidity, High Fatigue, Low Flow, PaintableInformation provided by Bhansali
Izod Impact, Notched 2.35 J/cm
<br>@Thickness 3.20 mm
4.41 ft-lb/in
<br>@Thickness 0.126 in
ASTM D256
Bhansali Engineering Abstron KU603 ABS Heat Resistant
High Impact, High RigidityInformation provided by Bhansali
Izod Impact, Notched 2.35 J/cm
<br>@Temperature 23.0 °C
4.41 ft-lb/in
<br>@Temperature 73.4 °F
ASTM D256
E-Polymers SEPAZ® LB30 PA6 LFT Resin
Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver..
Izod Impact, Notched 2.35 J/cm
<br>@Temperature -30.0 °C
4.41 ft-lb/in
<br>@Temperature -22.0 °F
ASTM D256
E-Polymers SEPAZ® LB30 PA6 LFT Resin
Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver..
Izod Impact, Notched 2.35 J/cm
<br>@Thickness 6.40 mm
4.41 ft-lb/in
<br>@Thickness 0.252 in
ASTM D-256
Bhansali Engineering Abstron IM-14G ABS Very High Rigidity Injection Molding Grade
Very High Rigidity, High Gloss, Medium Impact with excellent other mechanical propertiesInformation provided by Bhansali
Izod Impact, Notched 2.35 J/cm
<br>@Thickness 3.20 mm
4.41 ft-lb/in
<br>@Thickness 0.126 in
ASTM D256
Bhansali Engineering Abstron KU602 ABS Heat Resistant
High ImpactInformation provided by Bhansali
Izod Impact, Notched 2.35 J/cm
<br>@Thickness 6.40 mm,<br> Temperature 23.0 °C
4.41 ft-lb/in
<br>@Thickness 0.252 in,<br> Temperature 73.4 °F
ASTM D256
LG Chemical SG175G ABS, Super Surface Gloss, High Flow
Feature: Injection Molding, Super Surface Gloss, High FlowApplication: Electric & Electronic ProductsCAS No. 9003-56-9Information provided by LG Chemical
Copyright © lookpolymers.com All Rights Reserved