| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched | 1.50 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.81 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Flow; ASTM D256A |
| PolyOne Geon™ Vinyl Rigid Extrusion 87416 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
| Izod Impact, Notched | 1.50 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.81 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Flow; ASTM D256A |
| PolyOne Geon™ Vinyl Rigid Extrusion L0148 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: Finished part testing is required for ASTM E-84 certification. Note: The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by Po.. |
|||
| Izod Impact, Notched | 1.50 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.81 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Flow; ASTM D256A |
| PolyOne Geon™ Vinyl Rigid Extrusion L7416 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
| Izod Impact, Notched | 1.50 J/cm @Thickness 3.20 mm, Temperature -20.0 °C |
2.81 ft-lb/in @Thickness 0.126 in, Temperature -4.00 °F |
ISO 180/4A |
| Polimeri Europa Sinkral® B 532/E ABS Resin Sinkral B 532/E is an extrusion grade, which combines high toughness with good rigidity. Its rheological characteristics and good thermal stability are required for the production of large extruded .. |
|||
| Izod Impact, Notched | 1.50 J/cm @Temperature -30.0 °C |
2.81 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
| Ovation Polymers Nima™ NH PC143P Polycarbonate Non-Hal FR-PC with High impact and improved processabilityAll properties after 48hrs conditioning at 23°C/50% RH |
|||
| Izod Impact, Notched | 1.50 J/cm @Thickness 4.00 mm, Temperature -20.0 °C |
2.81 ft-lb/in @Thickness 0.157 in, Temperature -4.00 °F |
ISO 180 |
| Premix Thermoplastics PRE-ELEC® PE 1291 PRE-ELEC PE 1291 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129.. |
|||
| Izod Impact, Notched | 1.50 J/cm @Temperature 23.0 °C |
2.81 ft-lb/in @Temperature 73.4 °F |
double-gated; SABIC Method |
| SABIC Innovative Plastics Cycoloy® CX5640 PC+ABS (Europe-Africa-Middle East) Cycoloy* CX5640 is a all purpose PC+ABS blend specially developed for applications requiring weld line strength. High heat resistance combined with good flow, excellent impact and low temperature du.. |
|||
| Izod Impact, Notched | 1.50 J/cm @Temperature -30.0 °C |
2.81 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
| SABIC Innovative Plastics Lexan® EXL4019 PC (Europe-Africa-Middle East) Lexan* EXL4019 is an opaque 9% Glass Fiber (GF) reinforced polycarbonate (PC) siloxane copolymer resin for injection molding (IM) applications requiring improved stiffness. This resin also offers im.. |
|||
| Izod Impact, Notched | 1.50 J/cm @Temperature -30.0 °C |
2.81 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
| SABIC Innovative Plastics Lexan® ML6413 PC (Europe-Africa-Middle East) Lexan* ML6413 resin is an impact modified, flame retardant polycarbonate grade with Br- & Cl-free FR systems. It features improved light shielding capability with good flow, impact and thermal prope.. |
|||
| Izod Impact, Notched | 1.50 J/cm @Temperature -20.0 °C |
2.81 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
| LATI LATISTAT 43/7-02 Low Density Polyethylene (LDPE) Base Conductive Plastic
(discontinued **) Description: Latistat materials have low specific resistivity. They feature partial electrical conductivity. Selected functional additives give materials with low specific resistivity and reasonable.. |
|||
| Izod Impact, Notched | 1.50 J/cm @Temperature -30.0 °C |
2.81 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
| SABIC Innovative Plastics Xenoy® X4810 PBT+PC Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent.. |
|||
| Izod Impact, Notched | 1.50 J/cm @Temperature -30.0 °C |
2.81 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
| SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq.. |
|||
| Izod Impact, Notched | 1.50 J/cm @Temperature -30.0 °C |
2.81 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
| SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA (Asia Pacific) NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq.. |
|||
| Izod Impact, Notched | 1.50 J/cm @Temperature -30.0 °C |
2.81 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
| SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA (Europe-Africa-Middle East) NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq.. |
|||
| Izod Impact, Notched | 1.50 J/cm @Temperature 23.0 °C |
2.81 ft-lb/in @Temperature 73.4 °F |
Absolute Drying; ASTM-D256 |
| Toyobo GLAMIDE® T-663G50 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
| Izod Impact, Notched | 1.50 J/cm @Temperature -40.0 °C |
2.81 ft-lb/in @Temperature -40.0 °F |
Practical Use (Water Absorption 0.8%); ASTM-D256 |
| Toyobo GLAMIDE® T-663G50A MXD66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
| Izod Impact, Notched | 1.50 J/cm @Temperature 23.0 °C |
2.81 ft-lb/in @Temperature 73.4 °F |
Practical Use (Water Absorption 1.75%); ASTM-D256 |
| Toyobo GLAMIDE® T-665C30 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
| Izod Impact, Notched | 1.50 J/cm @Temperature -40.0 °C |
2.81 ft-lb/in @Temperature -40.0 °F |
Absolute Drying; ASTM-D256 |
| Toyobo GLAMIDE® TY-102ND Nylon/Elastomer GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
| Izod Impact, Notched | 1.50 J/cm @Temperature 23.0 °C |
2.81 ft-lb/in @Temperature 73.4 °F |
Absolute Drying; ASTM-D256 |
| Toyobo GLAMIDE® TY-592GHV 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
| Izod Impact, Notched | 1.50 J/cm @Temperature 0.000 °C |
2.81 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
| Cossa Polimeri ESTADIENE 0420 HHT Acrylonitrile Butadiene Styrene ABS for injection molding or extrusionVery high thermal resistance, good impact resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
| Izod Impact, Notched | 1.50 J/cm @Temperature 0.000 °C |
2.81 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
| Cossa Polimeri ESTADIENE 0425 GFS Acrylonitrile Butadiene Styrene, 13% Glass Filled ABS with 13% short glass fiberExcellent mechanical and thermal propertiesInformation provided by Cossa Polimeri S.r.l. |
|||
| Izod Impact, Notched | 1.50 J/cm @Temperature 0.000 °C |
2.81 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
| Cossa Polimeri ESTADIENE 1020 HHT Acrylonitrile Butadiene Styrene ABS with very high heat resistanceGood melt flow rate, good impact resistance, stiff, excellent surface appearance, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
| Izod Impact, Notched | 1.50 J/cm @Temperature 23.0 °C |
2.81 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
| Cossa Polimeri ESTADIENE 1515 HT Acrylonitrile Butadiene Styrene ABS with high thermal resistanceGood melt flow rate, good impact resistance, high gloss, with antistatic, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
| Izod Impact, Notched | 1.50 J/cm @Temperature 23.0 °C |
2.81 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
| Cossa Polimeri ESTAPROP H 05100 GFC Polypropylene, 50% Glass Filled PP homopolymer 50% chemically coupled glass fiberExcellent stiffness, excellent impact strengthInformation provided by Cossa Polimeri S.r.l. |
|||
| Izod Impact, Notched | 1.50 J/cm @Thickness 6.35 mm, Temperature -30.0 °C |
2.81 ft-lb/in @Thickness 0.250 in, Temperature -22.0 °F |
ASTM D256 |
| Diamond Polymers ABSPC 7030-HES ABS/PC Injection Molding Grade, High Impact Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
| Izod Impact, Notched | 1.50 J/cm @Temperature 23.0 °C |
2.81 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
| Carmel Olefins CAPILENE® SG 50 Polypropylene Impact Copolymer Description: CAPILENE® SG 50 is a low melt flow rate impact copolymer suitable for injection molding applications. It exhibits good stiffness combined with high impact strength.Applications: CAP.. |
|||
| Izod Impact, Notched | 1.50 J/cm @Temperature -40.0 °C |
2.81 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
| LATI LARIL 13-V1 Polyphenylene Oxide (PPOm) (UL94V-1)
(discontinued **) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||