| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched | 0.785 J/cm @Temperature -20.0 °C |
1.47 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
| PolyMirae Moplen EP300L Injection Molding Grade Polypropylene Moplen EP300L is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP300L is a block copolymer selected by customers for use in in.. |
|||
| Izod Impact, Notched | 0.785 J/cm @Temperature 23.0 °C |
1.47 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
| PolyMirae Moplen EP640S Injection Molding Grade Polypropylene Moplen EP640S is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP640S is a block copolymer particularly suitable for injection.. |
|||
| Izod Impact, Notched | 0.785 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
1.47 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
| LG Chemical HIPS 405AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 158725-44-1 and 1309-64-4Information provided by LG Chemical |
|||
| Izod Impact, Notched | 0.785 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.47 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
| LG Chemical HIPS 406AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Office Appliances (Parts of Printer or Copier)CAS: 9003-55-8, 25713-60-4 and 1309-64-4Information provided by LG Chemical |
|||
| Izod Impact, Notched | 0.785 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
1.47 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
| LG Chemical HIPS 410AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Office Appliances (Parts of Printer or Copier)CAS: 9003-55-8, 25713-60-4 and 1309-64-4Information provided by LG Chemical |
|||
| Izod Impact, Notched | 0.785 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
1.47 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
| LG Chemical HIPS 501S PS, Impact Modified Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: Refrigerator Food Holder, Food Container, Plastic Toy, Sheet or Film of Yot ReceptacleCAS: 9003-55-8Information provi.. |
|||
| Izod Impact, Notched | 0.785 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
1.47 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
| LG Chemical HIPS MI750L PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
| Izod Impact, Notched | 0.785 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
1.47 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
| LG Chemical LI931 Extrusion ASA Description: Low Gloss, Extrusion Application: Industrial Materials (Window Profile, Tile Etc)CAS: 26299-47-8 & 9003-54-7Information provided by LG Chemical |
|||
| Izod Impact, Notched | 0.785 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
1.47 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
|
| LG Chemical LUMILOY GN1306F Injection Molding FR Heat Resistant mPPO Uses include electric/electronic parts. |
|||
| Izod Impact, Notched | >= 0.785 J/cm @Thickness 6.40 mm, Temperature -30.0 °C |
>= 1.47 ft-lb/in @Thickness 0.252 in, Temperature -22.0 °F |
ASTM D256 |
| LG Chemical LUPOL TE5108H PP+Rubber+MF, High Impact Description: Injection Molding, PP+Rubber+MF, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia, Rear Bumper Step)Information provided by LG Chemical |
|||
| Izod Impact, Notched | >= 0.785 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
>= 1.47 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
| LG Chemical LUPOL HM3207 PP+MF20%, High Stiffness Description: Injection Molding, PP+MF20%, Good Weatherability, High StiffnessApplication: Automotive Interior Parts CAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
| Izod Impact, Notched | 0.785 J/cm @Thickness 3.17 mm |
1.47 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Samsung Cheil Industries Infino® AR-5300H PBT/ASA, 30% Glass Filled Information provided by Samsung Cheil Industries. |
|||
| Izod Impact, Notched | 0.785 J/cm @Thickness 6.35 mm |
1.47 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
| Samsung Cheil Industries Infino® GP-5300G PBT, Glass Filled Information provided by Samsung Cheil Industries. |
|||
| Izod Impact, Notched | 0.785 J/cm @Thickness 6.35 mm |
1.47 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
| Samsung Cheil Industries Infino® HN-3104 PC, 10% Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
| Izod Impact, Notched | 0.785 J/cm @Thickness 6.35 mm |
1.47 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
| Samsung Cheil Industries Infino® NH-1150HH PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
| Izod Impact, Notched | 0.785 J/cm @Thickness 3.17 mm |
1.47 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Samsung Cheil Industries Infino® NH-1150HH PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
| Izod Impact, Notched | 0.785 J/cm @Thickness 3.17 mm |
1.47 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Samsung Cheil Industries Infino® VB-5302GR PBT, 30% Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
| Izod Impact, Notched | 0.785 J/cm @Thickness 6.35 mm, Temperature -30.0 °C |
1.47 ft-lb/in @Thickness 0.250 in, Temperature -22.0 °F |
ASTM D256 |
| Samsung Cheil Industries Starex® MP-0670 ABS, Metal Plating Grade Information provided by Samsung Cheil Industries. |
|||
| Izod Impact, Notched | 0.785 J/cm @Thickness 3.17 mm |
1.47 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Samsung Cheil Industries Infino® AR-5300H PBT/ASA, 30% Glass Filled Information provided by Samsung Cheil Industries. |
|||
| Izod Impact, Notched | 0.785 J/cm @Thickness 6.35 mm |
1.47 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
| Samsung Cheil Industries Infino® GP-5300G PBT, Glass Filled Information provided by Samsung Cheil Industries. |
|||
| Izod Impact, Notched | 0.785 J/cm @Thickness 6.35 mm |
1.47 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
| Samsung Cheil Industries Infino® HN-3104 PC, 10% Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
| Izod Impact, Notched | 0.785 J/cm @Thickness 6.35 mm |
1.47 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
| Samsung Cheil Industries Infino® NH-1150HH PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
| Izod Impact, Notched | 0.785 J/cm @Thickness 3.17 mm |
1.47 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Samsung Cheil Industries Infino® NH-1150HH PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
| Izod Impact, Notched | 0.785 J/cm @Thickness 6.35 mm |
1.47 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
| Samsung Cheil Industries Starex® BF-0679P MABS, Unreinforced Scratch Resistant Scratch resistant material that is used for the exterior material of flat TVInformation provided by Samsung Cheil Industries. |
|||
| Izod Impact, Notched | 0.785 J/cm @Thickness 6.35 mm, Temperature -30.0 °C |
1.47 ft-lb/in @Thickness 0.250 in, Temperature -22.0 °F |
ASTM D256 |
| Samsung Cheil Industries Starex® MP-0670 ABS, Metal Plating Grade Information provided by Samsung Cheil Industries. |
|||
| Izod Impact, Notched | 0.785 J/cm @Thickness 6.35 mm |
1.47 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
| Samsung Cheil Industries Starex® BF-0679P MABS, Unreinforced Scratch Resistant Scratch resistant material that is used for the exterior material of flat TVInformation provided by Samsung Cheil Industries. |
|||
| Izod Impact, Notched | 0.785 J/cm @Thickness 3.17 mm |
1.47 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Samsung Cheil Industries Infino® VB-5302GR PBT, 30% Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
| Izod Impact, Notched | 0.785 J/cm @Temperature 23.0 °C |
1.47 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
| SCG Chemicals EL-Leneâ„¢ H570P High Density Polyethylene Pipe Resin Key Characteristics: High stiffness, good processingRecommended Applications: Corrugated pipes, non pressure pipes, conduit, sewage drainage pipesInformation provided by SCG Chemicals |
|||
| Izod Impact, Notched | 0.785 J/cm @Temperature 23.0 °C |
1.47 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
| SCG Chemicals EL-Proâ„¢ P740J Polypropylene Injection Molding Key Characteristics:Good flowabilityGood processabilityHigh stiffnessRecommended Applications:Automotive, motorcycle and electrical appliance parts that require good flowability such as automotive t.. |
|||