Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | >= 5.33 J/cm @Temperature 23.0 °C |
>= 9.99 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Tenite 360A4861316 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Izod Impact, Notched | >= 5.33 J/cm @Temperature 23.0 °C |
>= 9.99 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Tenite 360E2R30016 Cellulose Acetate Propionate, Natural, Trsp Applications:AppliancesPersonal Care and CosmeticsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss.. |
|||
Izod Impact, Notched | >= 5.33 J/cm @Temperature 23.0 °C |
>= 9.99 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Tenite 360E3V45516 Propionate Water Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Izod Impact, Notched | >= 5.33 J/cm @Temperature 23.0 °C |
>= 9.99 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Tenite 360E4861316 Cellulose Acetate Propionate, Clear, Trsp Applications:ProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. T.. |