Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 5.23 J/cm @Temperature 23.0 °C |
9.80 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® FXG1414T PC Copolymer (Europe-Africa-Middle East) PC-siloxane copolymer in special "Diamond Sparkle" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supp.. |
|||
Izod Impact, Notched | 5.23 J/cm @Temperature 23.0 °C |
9.80 ft-lb/in @Temperature 73.4 °F |
3.2 mm (0.125 in) notch |
Kraton® G1652 + PP blend + Talc (12/21/67) Unmodified polypropylene has high rigidity and good heat resistance, but poor impact resistance, especially at low temperatures. Blending KRATON D and G polymers with PP significantly improves the .. |
|||
Izod Impact, Notched | 5.23 J/cm @Temperature 23.0 °C |
9.80 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Tenite 307A4000018 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Izod Impact, Notched | 5.23 J/cm @Temperature 23.0 °C |
9.80 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Tenite 307E4000018 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Izod Impact, Notched | 5.23 J/cm @Temperature 23.0 °C |
9.80 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Tenite 380A3V32818 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Izod Impact, Notched | 5.23 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
9.80 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D-256 |
Axiall 8264 Rigid PVC, Extrusion Georgia Gulf 8264 is a rigid PVC pellet compound suited for applications where transparency is important. 8264 is widely used for clear films, sheets, and profile shapes in the packaging industry. .. |