Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 4.27 J/cm @Temperature -40.0 °C |
8.00 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Oxford Polymers 604-I Polycarbonate/Polybutylene Terephthalate (PBT) Alloy Polycarbonate/Polybutylene Terephthalate (PBT) AlloyInformation provided by Oxford Polymers. |
|||
Izod Impact, Notched | 4.27 J/cm @Temperature 23.0 °C |
8.00 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Noble Polymers Regis™ 285107 Thermoplastic Olefin (TPO) Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi.. |
|||
Izod Impact, Notched | 4.27 J/cm @Temperature -40.0 °C |
8.00 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Polymer Resources PC/TP-GP2 PC/Polyester Alloy High Impact, Excellent Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided b.. |
|||
Izod Impact, Notched | 4.27 J/cm @Temperature -40.0 °C |
8.00 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Polymer Resources PC/TP-GP2-[color]-UV PC/Polyester Alloy, UV-stabilized High Impact, Excellent Chemical Resistance, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Izod Impact, Notched | 4.27 J/cm @Temperature -34.4 °C |
8.00 ft-lb/in @Temperature -30.0 °F |
ASTM D256 |
Polymer Resources PC/TP-GP3-IM PC/Polyester Alloy, Impact Modified Superior Chemical Resistance, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provide.. |
|||
Izod Impact, Notched | 4.27 J/cm @Temperature 22.8 °C |
8.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PPX-GP3-IM Modified-PPO, Impact Modified Modified-Polyphenylene Oxide, Impact Modified, 235F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Izod Impact, Notched | 4.27 J/cm @Temperature -40.0 °C |
8.00 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Ravago Manufacturing Americas Hybrid B2026IU Polycarbonate + PBT Alloy Available in North America UV Stabilizer Good Impact Resistance RoHS Compliant Form: Pellets Processing Method: Injection Molding Information provided by Ravago |
|||
Izod Impact, Notched | 4.27 J/cm @Thickness 3.17 mm |
8.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LG Chemical Lupox® PBT-HI1002F Impact Modified, Flame Retardant PBT Alloy Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 4.27 J/cm @Thickness 3.17 mm, Temperature -30.0 °C |
8.00 ft-lb/in @Thickness 0.125 in, Temperature -22.0 °F |
ASTM D256 |
Lucent Polymers PC/PBT-1550 Polycarbonate+PBT, Improved Impact Resistance, Injection Grade Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Izod Impact, Notched | 4.27 J/cm @Temperature -30.0 °C |
8.00 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
MRC Polymers NAXALOYâ„¢ 770 ABS + PC Alloy Impact modifiedAvailable in Natural, Black, and GrayCan be Colored (Masterbatch)Low temperature ductility and impact modifiedCan be UV StabilizedInternal and external lubricant can be addedInformati.. |
|||
Izod Impact, Notched | 4.27 J/cm @Temperature -20.0 °C |
8.00 ft-lb/in @Temperature -4.00 °F |
ASTM D 256 |
MRC Polymers NAXALOYâ„¢ 770-NT137 ABS + PC Alloy Information provided by MRC Polymers Inc. |
|||
Izod Impact, Notched | 4.27 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
8.00 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6 IM 7050 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier, Nucleating Agent and LubricantFeatures: Heat Stabilized, Impact Modified, Nucleated and LubricatedInformation pro.. |
|||
Izod Impact, Notched | 4.27 J/cm @Temperature -40.0 °C |
8.00 ft-lb/in @Temperature -40.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Xenoy® 364 PBT This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 4.27 J/cm @Temperature -40.0 °C |
8.00 ft-lb/in @Temperature -40.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Asia Pacific) Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 4.27 J/cm @Temperature -40.0 °C |
8.00 ft-lb/in @Temperature -40.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Europe-Africa-Middle East) Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 4.27 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
8.00 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Plastiblend® PC/ABS 720 BK Availability: North AmericaForms: PelletsAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 4.27 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
8.00 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Plastiblend® PC/ABS FR 6206 Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 4.27 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
8.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Plastiblend® PC/PBT IM 1012 Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 4.27 J/cm @Temperature -40.0 °C |
8.00 ft-lb/in @Temperature -40.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Valox® 364 PBT Designed for outdoor telecommunications enclosure applications.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 4.27 J/cm @Thickness 6.35 mm, Temperature -30.0 °C |
8.00 ft-lb/in @Thickness 0.250 in, Temperature -22.0 °F |
ASTM D256 |
PlastxWorld CEVIAN® S1500 High Heat PC/ABS alloy These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Izod Impact, Notched | 4.27 J/cm @Thickness 3.17 mm |
8.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Chi Mei Polylac® PA-747R ABS - Extrusion Attach case and refrigerator |
|||
Izod Impact, Notched | 4.27 J/cm @Thickness 6.35 mm |
8.00 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Axiall 7450 Rigid PVC, Extrusion Georgia Gulf 7450 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: Excellent ToughnessSatin Surface AppearanceColorabilityChemical Res.. |
|||
Izod Impact, Notched | 4.27 - 5.87 J/cm @Thickness 3.17 mm, Temperature 0.000 °C |
8.00 - 11.0 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D-256 |
Axiall Suprel® SVA 9812 Rigid PVC, Extrusion Georgia Gulf Suprel® SVA 9812 Alloy is an extrusion grade thermoplastic designed for sheet or profile applications requiring high impact resistance. Key features of Suprel 9812 alloy are flame ret.. |